Latex sheet material, preparation method and latex mattress prepared from same
A latex sheet and latex technology, applied in the field of latex mattresses, can solve the problems of no therapeutic effect and achieve the effect of improving microcirculation and preventing allergic diseases and infectious diseases
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0046] The latex sheet of present embodiment 1 is mainly prepared from latex solution, negative oxygen ion powder and nano-silver, and the quality of negative oxygen ion powder is 3% of the quality of latex solution, and the quality of nano-silver is 3‰ of the quality of latex solution .
[0047] Specifically, the following preparation steps are included;
[0048] Add 1 kg of vulcanizing agent PDM, 1.5 kg of accelerator ZDMC-80, and 1 kg of anti-aging agent DNP into 30 kg of styrene-butadiene latex, mature for 24 hours, and then add foaming agent RAYNOLCH-2001 kg, gelling agent 1.5 kg and zinc oxide 2.5 kg to obtain a latex solution.
[0049] Add the negative oxygen ion powder and nano-silver into the latex solution, stir it fully by mechanical stirring, and then pump it onto the track of the shaped foaming machine. The thickness of the latex sponge sheet has been set at the joint of the track, and it is transported continuously Foam out the latex sponge sheet with the requir...
Embodiment 2
[0055] The latex sheet of present embodiment 2 is mainly prepared from latex solution, negative oxygen ion powder and nano-silver, and the quality of negative oxygen ion powder is 6% of the quality of latex solution, and the quality of nano-silver is 5‰ of the quality of latex solution .
[0056] Its preparation step has following difference on the basis of embodiment 1:
[0057] In this embodiment, the latex used is natural latex, and the latex mattress made of natural latex has the characteristics of high elasticity, shock absorption, resistance to compression fatigue, good bearing capacity, comfort and durability.
[0058] In the step of preparing latex solution, add vulcanizing agent PDM1kg, accelerator ZDMC-802kg, anti-aging agent DNP1kg into 30kg of natural latex, mature for 24 hours, then add foaming agent RAYNOLCH-2001kg, gelling agent 1.5kg and zinc oxide 2.5 kg to obtain a latex solution.
[0059] In the step of baking and setting, the infrared lamp tube is heated ...
Embodiment 3
[0065] The latex mattress of the present embodiment 1 is mainly prepared from latex solution, negative oxygen ion powder and nano-silver, and the quality of negative oxygen ion powder is 3% of the latex solution quality, and the quality of nano-silver is 4‰ of the latex solution quality .
[0066] Its preparation step has following difference on the basis of embodiment 1:
[0067] In this embodiment, the latex is a mixed latex composed of natural latex and styrene-butadiene latex at a volume ratio of 1:1.
[0068] In the step of preparing latex solution, add vulcanizing agent PDM3kg, accelerator ZDMC-805kg, anti-aging agent DNP4kg in 60kg mixed latex, mature for 72 hours, then add foaming agent RAYNOLCH-2005kg, gelling agent 4kg and zinc oxide 5kg, A latex solution is obtained.
[0069] In the step of baking and setting, the infrared lamp tube is heated to 70°C, and the foamed latex sponge sheet is irradiated for 30 minutes to make it mature and set.
[0070] In the punchin...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com