Embodiment 1
[0018] A scrub-resistant and antibacterial interior wall latex paint, its raw materials include by weight: 40 parts of modified PVA, 12 parts of methyl methacrylate, 1 part of polymethyl methacrylate, 16 parts of light calcium carbonate, and 5 parts of talcum powder , Lithopone 20 parts, calcined kaolin 10 parts, hydroxyethyl cellulose 0.3 parts, dispersant SN-50400.5 parts, dispersant SN-50270.2 parts, multifunctional additive AMP-950.1 parts, alcohol ester twelve 0.8 parts, 0.2 parts of defoamer NXZ, 1.0 parts of negative ion-antibacterial additive, 0.3 parts of sodium polyphosphate, 0.5 parts of leveling agent, 10.5 parts of nano-stain resistant agent NZW-1.8 parts of propylene glycol, 5-chloro-2-methyl -0.3 parts of 4-isothiazolin-3-one, 50 parts of deionized water;
Embodiment 2
[0020] A scrub-resistant antibacterial interior wall latex paint, its raw materials include by weight: 60 parts of modified PVA, 5 parts of methyl methacrylate, 6 parts of polymethyl methacrylate, 6 parts of light calcium carbonate, 15 parts of talcum powder , 10 parts of lithopone, 15 parts of calcined kaolin, 0.1 part of hydroxyethyl cellulose, 0.7 parts of dispersant SN-5040, 0.1 part of dispersant SN-50270, 0.2 parts of multifunctional additive AMP-950, 0.5 parts of alcohol ester twelve, 0.4 parts of defoaming agent NXZ, 0.8 parts of negative ion-antibacterial additive, 0.5 parts of sodium polyphosphate, 0.3 parts of leveling agent, 11.0 parts of nano-stain resistant agent NZW-11.0 parts, 0.5 parts of propylene glycol, 5-chloro-2-methyl -1.2 parts of 4-isothiazolin-3-one, 35 parts of deionized water;
[0021]The modified PVA is prepared according to the following process: add 12 parts of polyvinyl alcohol and 3 parts of propylene glycol methyl ether into 30 parts of water ...
Embodiment 3
[0026] A scrub-resistant antibacterial interior wall latex paint, its raw materials include by weight: 45 parts of modified polyvinyl alcohol, 10 parts of methyl methacrylate, 2 parts of polymethyl methacrylate, 14 parts of light calcium carbonate, talc 7 parts of powder, 18 parts of lithopone, 11 parts of calcined kaolin, 0.2 parts of hydroxyethyl cellulose, 0.6 parts of dispersant SN-5040, 0.2 parts of dispersant SN-50270, 0.1 part of multifunctional additive AMP-950, alcohol ester dodecane 0.7 parts, 0.3 parts of defoaming agent NXZ, 0.9 parts of anion-antibacterial additives, 0.3 parts of sodium polyphosphate, 0.5 parts of leveling agent, 10.6 parts of nano stain resistance agent NZW-1.4 parts of propylene glycol, 5-chloro-2 - 0.5 parts of methyl-4-isothiazolin-3-one, 45 parts of deionized water;
[0027] The modified PVA is prepared according to the following process: add 18 parts of polyvinyl alcohol and 1 part of propylene glycol methyl ether to 50 parts of water and so...
PUM
Property | Measurement | Unit |
---|---|---|
density | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com