A phosphorescent material and three-coordination technology, which is applied in the field of luminescent materials and organic electroluminescent materials, can solve the problems of suppressing excited state distortions that are not ideal, limited, and luminous efficiency does not meet the requirements of the application, and achieve good phosphorescent emission performance , The equipment is simple, and the effect of promoting inter-system crossing
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] Preparation of a large amount of phosphorescent complex CuBr (DPPBP) (DAF) microcrystalline samples: Weigh 0.5 mmol of CuBr and dissolve it in 25 mL of acetonitrile, weigh 0.5 mmol of bis(diphenylphosphine) biphenyl ligand and dissolve it in 15 mL of ethanol , mix the two solutions, and stir to make the coordination reaction fully occur to obtain a colorless solution A; then weigh 0.5mmol of DAF ligand and dissolve it in 15mL of ethanol, then add this solution to the above solution A, and Stir to make the coordination reaction fully occur, and finally the obtained yellow reaction liquid is rotary evaporated to remove all solvents, and vacuum-dried to obtain yellow granular fine crystal powder as the product, with a yield of 98% (calculated as Cu). Elemental Analysis Calculated (C35H27N2PCuBr): C, 64.67%; H, 4.19%; N, 4.31%. Experimental values: C, 63.82%; H, 4.08%; N, 4.22%. IR (KBr pellet, cm -1 ): 3428m, 3051m, 2921w, 1583m, 1571m, 1479m, 1463m, 1434s, 1412s, 1391m,...
Embodiment 2
[0032] Synthesis of single crystal of phosphorescent cuprous complex CuBr(DPPBP)(DAF): Dissolve CuBr (0.015g, 0.1mmol) in 5ml of acetonitrile, ligand 4,5-diazafluorene (0.017g, 0.1mmol) and bis(diphenylphosphine)biphenyl (0.035g, 0.1mmol) were dissolved in 5ml of ethanol, after complete dissolution, the two were mixed, stirred rapidly for 5min and then filtered to obtain a yellow clear solution. The filtrate was placed in a 25ml beaker, covered with a plastic wrap, pierced with a needle and crystallized by volatilization. After about 3 days, yellow blocky crystals were obtained. A yellow bulk transparent crystal with a size of 0.28mm×0.15mm×0.10mm was selected for X-ray single crystal diffraction structure test. The molecular structure of the compound is shown in the attached figure 1 , and its unit cell packing structure is shown in the attached figure 2 .
[0033] A series of performance tests were carried out on pure-phase crystal samples of phosphorescent cuprous comp...
PUM
Property | Measurement | Unit |
---|---|---|
luminous efficiency | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com