A technology of EPDM and high-density polyethylene, which is applied in the field of composite conductive material preparation, can solve the problems of damage to the comprehensive mechanical properties and processing and molding properties of the matrix polymer material, and increase the cost, so as to reduce the decline of other properties and improve the The effect of processability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] Add 25 grams of aniline monomer to 75 grams of EPDM powder and stir evenly. Under the conditions of ultrasonic power of 100W and frequency of 120kHz at 30°C, it is subjected to ultrasonic radiation treatment. The treatment time is 1.0 hour. Diffusion into the EPDM powder, causing it to swell.
[0020] Immerse 20 grams of swollen EPDM rubber powder into 1000 grams of 0.5mol / L p-toluenesulfonic acid aqueous solution, control the temperature at 20°C, and dissolve 20 grams of ammonium persulfate in 0.5mol / L p-toluenesulfonic acid solution. 500 grams of p-toluenesulfonic acid aqueous solution was added slowly, and the reaction time was 1.0 hour. After the reaction, the material was washed with water and dried to obtain EPDM / polyaniline composite conductive powder.
[0021] Put 35 grams of EPDM rubber / polyaniline composite conductive powder and 65 grams of polypropylene into a high-speed mixer, control the mixing temperature at 40 ° C, mix evenly, use a twin-screw extruder to...
Embodiment 2
[0023] Add 25 grams of aniline monomer to 75 grams of EPDM powder and stir evenly. Under the conditions of ultrasonic power of 200W and frequency of 20kHz at 20°C, it is subjected to ultrasonic radiation treatment. The treatment time is 0.5 hours. Diffusion into the EPDM powder, causing it to swell.
[0024] Immerse 30 grams of swollen EPDM rubber powder into 1000 grams of 1.0mol / L p-toluenesulfonic acid aqueous solution, control the temperature at 0°C, and dissolve 60 grams of ammonium persulfate in 1.0mol / L p-toluenesulfonic acid solution. 500 grams of p-toluenesulfonic acid aqueous solution was added slowly, and the reaction time was 10.0 hours. After the reaction, the material was washed with water and dried to obtain EPDM / polyaniline composite conductive powder.
[0025] Put 40 grams of EPDM / polyaniline composite conductive powder and 40 grams of high-density polyethylene into a high-speed mixer, control the mixing temperature at 60°C, mix evenly, and use a twin-screw ext...
Embodiment 3
[0027] Add 40 grams of aniline monomer to 60 grams of EPDM powder and stir evenly. Under the conditions of ultrasonic power of 3000W and frequency of 59kHz at 15°C, it is subjected to ultrasonic radiation treatment. The treatment time is 1.5 hours. Diffusion into the EPDM powder, causing it to swell.
[0028] Immerse 60 grams of EPDM rubber powder after swelling into 1000 grams of 1.0mol / L p-dodecylbenzenesulfonic acid aqueous solution, control the temperature at 10°C, dissolve 0.5mol / L of 120 grams of ammonium persulfate 500 grams of p-toluenesulfonic acid aqueous solution of L was slowly added, and the reaction time was 2.0 hours. After the reaction, the material was washed with water, and dried to obtain EPDM / polyaniline composite conductive powder.
[0029]Put 50 grams of EPDM rubber / polyaniline composite conductive powder and 50 grams of high-density polyethylene into a high-speed mixer, control the mixing temperature at 50°C, mix evenly, and use a twin-screw extruder to ...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com