A geothermal system pipeline descaling agent and preparation method thereof
A descaling agent and pipeline technology, applied in the field of geothermal system pipeline descaling agent and its preparation, can solve the problem of unsuitable floor heating system pipeline descaling, etc., achieves inhibition of re-aggregation, good descaling effect, and remarkable descaling effect Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] All materials selected are commercially available. The geothermal system pipeline descaling agent of the present invention includes 8 parts of metal material protection agent copper sulfate powder, 14 parts of dissolving enzyme, 18 parts of synergist sodium citrate, 48 parts of acetic acid, 6 parts of sterilizing agent silver sulfate, corrosion inhibitor 3 parts of benzotriazole and 3 parts of antiscalant diaminomonocarboxylic acid.
[0027] During the preparation process, weigh each component in proportion, add copper sulfate powder, sodium citrate, and benzotriazole in turn to acetic acid at room temperature and stir for about 15 minutes, and stir evenly; let stand for 2 hours, add silver sulfate and stir for about 10 minutes, until stirred Evenly, then add diaminomonocarboxylic acid and lysozyme in sequence, stir at high speed for 12 minutes, and let stand for 1 hour to obtain the target product. The descaling effect data of the descaling agent are shown in Table 1....
Embodiment 2
[0029] All materials selected are commercially available. The geothermal system pipeline descaling agent of the present invention comprises 6 parts of manganese sulfate powder of metal material protection agent, 13 parts of dissolving enzyme, 16 parts of synergist zinc carbonate, 55 parts of acetic acid, 5 parts of sterilizing agent zinc sulfate, 10 parts of corrosion inhibitor 3 parts of hexaalkylamine and 2 parts of antiscalant p-hydroxycinnamic acid.
[0030] During the preparation process, weigh each component in proportion, add manganese sulfate powder, zinc carbonate, and hexadecylamine in turn to acetic acid at room temperature, stir for about 10 minutes, and stir evenly; let it stand for 2.5 hours, add zinc carbonate, and stir for about 10 minutes until it is stirred Evenly, then add p-hydroxycinnamic acid and lysozyme in sequence, stir at high speed for 12 minutes, and let stand for 1 hour to obtain the target product. The descaling effect data of the descaling agent...
Embodiment 3
[0032] All materials selected are commercially available. The geothermal system pipeline descaling agent of the present invention includes 6 parts of metal material protection agent potassium iodide powder, 13 parts of dissolving enzyme, 16 parts of synergist zinc phosphate, 55 parts of carbonic acid, 5 parts of sterilizing agent silver carbonate, corrosion inhibitor benzo 3 parts of triazole and 2 parts of antiscalant hydroxycitric acid.
[0033] During the preparation process, weigh each component in proportion, add potassium iodide powder, zinc phosphate, and benzotriazole to carbonic acid at room temperature and stir for about 10 minutes, and stir evenly; let it stand for 1.5 hours, add silver carbonate and stir for about 10 minutes, until it is evenly stirred , then sequentially added hydroxycitric acid and lysozyme, stirred at high speed for 12 minutes, and stood still for 1 hour to obtain the target product. The descaling effect data of the descaling agent are shown in...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com