A technology of functional materials and royal acid, applied in the direction of material separation, analytical materials, chemical instruments and methods, etc., can solve the problems of uneven particle size, low mass transfer speed, poor rigidity, etc., achieve uniform particle size and improve dispersibility , the effect of high selection specificity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0019] The invention discloses a method for preparing a functional material for adsorbing royal acid. A bulk polymerization method is used to prepare a molecularly imprinted polymer with royal acid as a template molecule. Dissolve 0.186g of royal acid in 10mL of methanol, and add 421μL of 4-vinylpyridine, 1514.7mg of N,N'-methylenebisacrylamide and 50mg of azobisisobutyronitrile in sequence. The reacted solution was purged with nitrogen gas for 10 minutes to remove oxygen, then placed in a water bath at 55° C., and thermally initiated polymerization for 24 hours. After the reaction, the mixed solution of methanol and glacial acetic acid with a volume ratio of 9:1 was Soxhlet-extracted for 24 hours, and methanol was used as solvent for 12 hours to wash off the residual glacial acetic acid, and vacuum-dried at 50°C to obtain the royal acid molecularly imprinted polymer .
[0020] Accurately weigh 150 mg of the powdered royal acid adsorption material synthesized in Example 1, an...
Embodiment 2
[0022] The invention discloses a method for preparing a functional material for adsorbing royal acid. A bulk polymerization method is used to prepare a molecularly imprinted polymer with royal acid as a template molecule. Dissolve 0.3 g of royal acid in 16 mL of methanol, and add 674 μL of 4-vinylpyridine, 2424 mg of N, N'-methylenebisacrylamide and 80 mg of azobisisobutyronitrile in sequence. The reacted solution was purged with nitrogen gas for 10 minutes to remove oxygen, then placed in a water bath at 55° C., and thermally initiated polymerization for 24 hours. After the reaction, the mixed solution of methanol and glacial acetic acid with a volume ratio of 9:1 was Soxhlet-extracted for 24 hours, and methanol was used as solvent for 12 hours to wash off the residual glacial acetic acid, and vacuum-dried at 50°C to obtain the royal acid molecularly imprinted polymer .
[0023] Accurately weigh 150 mg of the powdered royal acid adsorption material synthesized in Example 2, ...
PUM
Property | Measurement | Unit |
---|---|---|
adsorption capacity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com