Novel solid sterilizing and disinfecting material, and preparation and application thereof
A technology of sterilization and disinfection and new materials, applied in the field of materials, can solve the problems of uselessness of new materials, and achieve the effect of rapid process and convenient use.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0034]Mix 45Kg of quaternary ammonium salt (benzalkonium chloride) with 15Kg of polyamine (ethylenediamine) at about 60°C, heat up to 190-210°C at a speed of 10°C / 15min, react for 40-50 minutes, and then mix 20Kg of guanidine Salt (guanidine carbonate) is added and mixed, and when the temperature is lowered to 125-130°C, 20Kg of cetyl alcohol polyoxyethylene ether and other raw materials are added, mixed for 30 minutes, and finally the mixed raw materials are put into a granule extruder to granulate to obtain a solid sterilizing product. Material "XS-1".
Embodiment 2
[0036] 33Kg of quaternary ammonium salt (dodecyl dimethyl benzyl ammonium chloride) and 25Kg of polyamine (hexamethylenetetramine) are mixed at about 60°C, and the temperature is raised to 190-210°C at a speed of 10°C / 15min. React for 40-50 minutes, then add 17Kg of guanidine salt (guanidine nitrate) for mixing, then add 25Kg of cetyl alcohol polyoxyethylene ether and other raw materials when the temperature is lowered to 125-130°C, mix for 30 minutes, and finally put the mixed raw materials into the granule extrusion Plastic machine granulation to obtain solid sterilization and disinfection new material "XS-2".
Embodiment 3
[0038] Mix 50Kg of quaternary ammonium salt (benzalkonium bromide) and 20Kg of polyamine (1-6 hexamethylenediamine) at about 60°C, heat up to 190-210°C at a speed of 10°C / 15min, react for 40-50 minutes, and then Add 8Kg of guanidine salt (guanidine hydrochloride) and mix, then add 22Kg of cetyl alcohol polyoxyethylene ether and other raw materials when the temperature is lowered to 125-130°C, mix for 30 minutes, and finally put the mixed raw materials into a granule extruder for granulation to obtain solid sterilization Sterilized new material "XS-3".
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com