Embodiment 1
[0008] 24 parts of lithium silicate, 20 parts of graphite balls, 16 parts of vanadium trioxide, 10 parts of azodicarbonamide, 8 parts of zinc oxide, 4 parts of benzoyl peroxide, 12 parts of dibutyl phthalate, phosphoric acid 10 parts of triphenyl ester, 4 parts of isopropyl acrylate, 12 parts of epoxy resin, 8 parts of butyl acetate, 4 parts of ethylene glycol, 2 parts of ethylene glycol monohexyl ether, 4 parts of dimethylethanolamine, cobalt acid carbonate Put 4 parts of calcium into the reactor, stir continuously, heat to 65°C after mixing completely, and get the product after uniform stirring.
Embodiment 2
[0010] 30 parts of lithium silicate, 25 parts of graphite balls, 17 parts of vanadium trioxide, 15 parts of azodicarbonamide, 10 parts of zinc oxide, 8 parts of benzoyl peroxide, 15 parts of dibutyl phthalate, phosphoric acid 15 parts of triphenyl ester, 6 parts of isopropyl acrylate, 14 parts of epoxy resin, 10 parts of butyl acetate, 8 parts of ethylene glycol, 5 parts of ethylene glycol monohexyl ether, 6 parts of dimethylethanolamine, cobalt acid carbonate Put 5 parts of calcium into the reactor, stir continuously, heat to 65°C after mixing completely, and get the product after uniform stirring.
Embodiment 3
[0012] 36 parts of lithium silicate, 30 parts of graphite balls, 18 parts of vanadium trioxide, 20 parts of azodicarbonamide, 12 parts of zinc oxide, 12 parts of benzoyl peroxide, 18 parts of dibutyl phthalate, phosphoric acid 20 parts of triphenyl ester, 8 parts of isopropyl acrylate, 16 parts of epoxy resin, 12 parts of butyl acetate, 12 parts of ethylene glycol, 8 parts of ethylene glycol monohexyl ether, 8 parts of dimethylethanolamine, cobalt acid carbonate Put 6 parts of calcium into the reactor, stir continuously, heat to 65°C after mixing completely, and get the product after uniform stirring.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com