A kind of asphalt pavement reinforcement material
A technology for reinforcing material and asphalt pavement, applied in the field of additives for improving the performance of asphalt pavement, can solve the problems of high price of chemical fibers, difficult to achieve reinforcement and toughening, complicated production process, etc., and achieves increased consistency and workability of construction. , Improve anti-aging ability, the effect of easy availability of raw materials
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0015] A kind of asphalt pavement reinforcing material, its raw material components include by weight percentage:
[0016]
[0017] The waxy material on the surface layer of the above-mentioned cotton stalk fiber is removed through separation.
[0018] A kind of preparation method of asphalt pavement reinforcing material: respectively add polyester fiber, cotton stalk fiber, basalt fiber, polyethylene, carbon black in the mixer according to the above-mentioned ratio, stir for 3 minutes and obtain this asphalt pavement reinforcing material; First add asphalt pavement reinforcement materials and aggregates into the asphalt mixer, mix for 2 minutes, then add asphalt and wet mix for 1 minute, and it is ready.
Embodiment 2
[0020] A kind of asphalt pavement reinforcing material, its raw material components include by weight percentage:
[0021]
[0022]
[0023] The waxy material on the surface layer of the above-mentioned cotton stalk fiber is removed through separation.
[0024] A kind of preparation method of asphalt pavement reinforcing material: respectively add polyester fiber, cotton stalk fiber, basalt fiber, polyethylene, carbon black in the mixer according to the above-mentioned proportion, stir for 5 minutes and obtain this asphalt pavement reinforcing material; First add asphalt pavement reinforcement materials and aggregates into the asphalt mixer, mix for 2 minutes, then add asphalt and wet mix for 1 minute, and it is ready.
Embodiment 3
[0026] A kind of asphalt pavement reinforcing material, its raw material components include by weight percentage:
[0027]
[0028] The waxy material on the surface layer of the above-mentioned cotton stalk fiber is removed through separation.
[0029] A kind of preparation method of asphalt pavement reinforcing material: respectively add polyester fiber, cotton stalk fiber, basalt fiber, polyethylene, carbon black in the mixer according to the above-mentioned proportion, stir for 5 minutes and obtain this asphalt pavement reinforcing material; First add asphalt pavement reinforcement materials and aggregates into the asphalt mixer, mix for 2 minutes, then add asphalt and wet mix for 1 minute, and it is ready.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com