Water-repellent finishing method of clothes
A water-repellent finishing and clothing technology, which is applied in fiber processing, textiles and papermaking, etc., can solve the problems of poor water-repellent durability of clothes and achieve good durability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] A method for water-repellent finishing of clothes, comprising the steps of:
[0021] 1) Mix 23 parts of water, 1.2 parts of polyethylene glycol distearate, 2.3 parts of acrylic resin, 3.4 parts of polyvinylpyrrolidone, 4.5 parts of triethanolamine, and then slowly add 7.8 parts of anionic polyacrylamide, 1.2 parts of poly Oxyethylene ether, 6.7 parts of HPC-1 finishing agent, 8.9 parts of dimethylolethylene urea, and 1.2 parts of glyceryl monostearate were fed within 40 minutes, and continued to mix for 2 hours to obtain an impregnation solution;
[0022] 2) Pad the clothes in the dipping solution, the pressure is 2.5 MPa, the liquid retention rate is 73%, and after drying, keep the clothes at 145°C for 2.5 hours.
Embodiment 2
[0024] A method for water-repellent finishing of clothes, comprising the steps of:
[0025] 1) Mix 23 parts of water, 2 parts of polyethylene glycol distearate, 3 parts of acrylic resin, 4 parts of polyvinylpyrrolidone, and 5 parts of triethanolamine, and then slowly add 8 parts of anionic polyacrylamide, 2 parts of poly Oxyethylene ether, 7 parts of HPC-1 finishing agent, 9 parts of dimethylolethylene urea, and 2 parts of glyceryl monostearate were fed within 40 minutes, and continued to mix for 2 hours to obtain an impregnation solution;
[0026] 2) Pad the clothes in the dipping solution, the pressure is 2.5 MPa, the liquid retention rate is 73%, and after drying, keep the clothes at 145°C for 2.5 hours.
Embodiment 3
[0028] A method for water-repellent finishing of clothes, comprising the steps of:
[0029] 1) Mix 23 parts of water, 1 part of polyethylene glycol distearate, 2 parts of acrylic resin, 3 parts of polyvinylpyrrolidone, and 4 parts of triethanolamine, and then slowly add 7 parts of anionic polyacrylamide and 1 part of poly Oxyethylene ether, 6 parts of HPC-1 finishing agent, 8 parts of dimethylolethylene urea, and 1 part of glyceryl monostearate were fed within 40 minutes, and continued to mix for 2 hours to obtain an impregnating solution;
[0030] 2) Pad the clothes in the dipping solution, the pressure is 2.5 MPa, the liquid retention rate is 73%, and after drying, keep the clothes at 145°C for 2.5 hours.
[0031]
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.