[0037] In a specific embodiment of the method for preparing sterilization bedding for pets of the present invention, the preparation method includes the following steps:
[0038] (1) Manufacturing water storage particles: crushing, pulping, extruding, granulating and drying paper;
[0039] (2) Water mixing: Mix water on the surface of the water storage particles, the weight of which is 20%-30% of the weight of the water storage particles;
[0040] (3) Manufacturing polymer water-absorbing coating: take wood pulp powder, mix with polymer water-absorbing resin, and mix well;
[0041] (4) Coating: Mix the materials of steps (2) and (3), put them into the sugar coating machine and rotate, so that a coating layer is evenly adhered to the water storage particles;
[0042] (5) Drying;
[0043] Copper sulfate is added in step (1) pulping or / and step (3) when manufacturing the polymer water-absorbing coating layer, and the addition amount of copper sulfate is 0.1%-0.2% of the dry weight of the wa...
Embodiment 1
[0050] First, make water-storing particles: crush and pulp 1000 kg of paper with a pulper; then squeeze the material with a pulp squeezer until there is no more water to squeeze out; then use a pellet extruder to pelletize; and finally Granule dryer drying.
[0051] Then water mixing: After atomizing the water with a sprayer, spray it evenly on the surface of the water storage particles in the previous step, and the water mixing weight is 20% of the weight of the water storage particles;
[0052] Manufacture of polymer water-absorbing coating: take 62.5 kg of wood pulp powder for papermaking, mix with 1100 kg of acrylic polymer water-absorbing resin (250 mesh polyacrylic polymer water-absorbing resin 68.75 kg, 300 mesh polyacrylic polymer water-absorbing resin 68.75 kg), add 2 kg of copper sulfate and mix well. The ambient air humidity in the production process of this step is required to be lower than 40%. If the above-mentioned uniformly mixed polymer water-absorbing coating mat...
Embodiment 2
[0055] First, make water storage particles: crush 1,000 kg of paper with a pulper, add 1 kg of copper sulfate, and then make pulp; then use a pulp squeezer to squeeze the material until there is no more water to squeeze out; then use Pelletizing by pellet extruder; finally drying with pellet dryer.
[0056] Then water mixing: After atomizing the water with a sprayer, spray it evenly on the surface of the water storage particles in the previous step, and the water mixing weight is 30% of the weight of the water storage particles;
[0057] Manufacture of polymer water-absorbing coating: take wood pulp board and pulverize it into wood pulp powder with a grinder. The water content of wood pulp board does not exceed 10%, and it is mixed with acrylic polymer water-absorbing resin 1000 kg (250 mesh polyacrylic high 68.75 kilograms of molecular water-absorbing resin and 68.75 kilograms of 300-mesh polyacrylic polymer water-absorbing resin), mix well. The ambient air humidity in the produc...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com