Preparation method of solvent-type polystyrene modified asphalt waterproof paint

A technology for modifying asphalt and polystyrene, which is applied in asphalt coatings, coatings, etc., can solve the problems of high toxicity of tar gas, short construction period, poor environmental protection, etc., and achieves convenient and simple preparation, low equipment investment, and good use effect Effect

Inactive Publication Date: 2014-10-22
ANHUI PIONEER DOOR IND TECH
View PDF5 Cites 4 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0002] Waterproof coating refers to the coating used to prevent water intrusion and leakage. The waterproof film formed after curing of the waterproof coating has certain extensibility, elasticity, crack resistance, impermeability and weather resistance, which can play a role in waterproofing and waterproofing. Infiltration and protection, waterproof coatings have good temperature adaptability, easy operation, and easy repair and maintenance. There are two types of waterproof materials on the market: one is polyurethane waterproof coatings, which are generally made of polyurethane and coal. Tar is made as a raw material, and the tar gas it volatilizes is highly toxic and not easy to remove, so it was banned in China in 2000. The polyurethane waterproof coating that is still on the market uses pitch instead of coal tar as a raw material, but When using this kind of paint, it is generally diluted with organic solvents such as toluene and xylene, so it is also toxic; at the same time, it is inconvenient to construct, the overall cost is high, the construction period is short and long, and the environmental protection is relatively poor, but even with so many However, due to the lack of technology for the production of waterproof coatings at present, the degree of choice is very low. Most of the waterproof coatings used in the market are still this type of waterproof coatings.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Preparation method of solvent-type polystyrene modified asphalt waterproof paint
  • Preparation method of solvent-type polystyrene modified asphalt waterproof paint
  • Preparation method of solvent-type polystyrene modified asphalt waterproof paint

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0021] A solvent-based polystyrene modified asphalt waterproof coating is composed of the raw materials of the following components:

[0022]

[0023] The method for preparing solvent-based polystyrene modified asphalt waterproof coating of the present invention comprises the following processing steps:

[0024] a. Choose a mixing tank, pour the xylene and dichloropropane in the raw material into the mixing tank according to the formula amount and mix evenly, then put the polystyrene in the raw material into it, start stirring until it is completely dissolved and then set aside.

[0025] b. Select a heating and dissolving kettle, put the petroleum pitch in the raw material into it according to the formula amount, start heating until the temperature is 130-150°C, and start dehydration.

[0026] c. After the dehydration of the reactants in the dissolution kettle in step b is completed, all the rosin water, dibutyl phthalate, dioctyl phthalate, cresol and large white powder in...

Embodiment 2

[0029] A solvent-based polystyrene modified asphalt waterproof coating is composed of the raw materials of the following components:

[0030]

[0031] The method for preparing solvent-based polystyrene modified asphalt waterproof coating of the present invention comprises the following processing steps:

[0032] a. Choose a mixing tank, pour the xylene and dichloropropane in the raw material into the mixing tank according to the formula amount and mix evenly, then put the polystyrene in the raw material into it, start stirring until it is completely dissolved and then set aside.

[0033] b. Select a heating and dissolving kettle, put the petroleum pitch in the raw material into it according to the formula amount, start heating until the temperature is 130-150°C, and start dehydration.

[0034] c. After the dehydration of the reactants in the dissolution kettle in step b is completed, all the rosin water, dibutyl phthalate, dioctyl phthalate, cresol and large white powder in...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a preparation method of a solvent-type polystyrene modified asphalt waterproof paint, and relates to the technical field of chemical engineering. The paint is composed of the following raw materials in parts by weight: 7.9 to 8.1 parts of polystyrene, 24.0 to 24.2 parts of petroleum asphalt, 14.0 to 14.2 parts of xylene, 22.0 to 22.2 parts of dichloropropane, 1.1 to 1.3 parts of methylphenol, 14.0 to 14.2 parts of talcum powder, 2.3 to 2.5 parts of plasticizer, 5.9 to 6.1 part of stuffing material, and 7.9 to 8.1 parts of solvent oil. The preparation method has the advantages of simpleness, convenience, available raw materials, little equipment investment, and convenient operation. The prepared solvent-type polystyrene modified asphalt waterproof paint has the advantages of environment-friendliness, no pollution, high purity, good using effect, strong high-temperature resistant performance, safety, and reliability.

Description

technical field [0001] The invention relates to the technical field of chemical industry, in particular to a method for preparing a solvent-based polystyrene modified asphalt waterproof coating. Background technique [0002] Waterproof coating refers to the coating used to prevent water intrusion and leakage. The waterproof film formed after curing of the waterproof coating has certain extensibility, elasticity, crack resistance, impermeability and weather resistance, which can play a role in waterproofing and waterproofing. Infiltration and protection, waterproof coatings have good temperature adaptability, easy operation, and easy repair and maintenance. There are two types of waterproof materials on the market: one is polyurethane waterproof coatings, which are generally made of polyurethane and coal. Tar is made as a raw material, and the tar gas it volatilizes is highly toxic and not easy to remove, so it was banned in China in 2000. The polyurethane waterproof coating ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C09D195/00C09D125/06C09D7/12
Inventor 徐骏珂徐根运候飞虎王君
Owner ANHUI PIONEER DOOR IND TECH
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products