Rubber glove with antimicrobial function
A rubber glove and functional technology, applied in the field of surgical gloves, can solve the problems of hindering the speed of wound healing, no skin care, no maintenance, etc., to avoid allergic problems, avoid poor tensile properties, and avoid allergic symptoms.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0027] A kind of rubber glove with antibacterial function, wherein, described rubber latex is made up of following composition, by weight:
[0028]
[0029] The antibacterial active ingredient is composed of Luo Han Guo extract and Centella asiatica extract with a weight ratio of 1:2.
[0030] Its preparation method is as follows:
[0031] A, prepare the rubber latex that dipping is used, with natural rubber, emulsified liquid paraffin, colloidal sulfur, zinc oxide, promotor ZDBC, promotor ZMBT, antibacterial active ingredient, fully mix, adjust solid content to be 25-32%;
[0032] B, after the mold is dried, impregnate the coagulant first, and the coagulant is calcium nitrate or calcium chloride solution of 15% by weight;
[0033] C. Dry the mold, then dip the mold into the rubber latex prepared above, then crimp, then immerse in warm water at 45°C for 2 minutes, take it out, and dry it at a high temperature of 140°C for 20 minutes;
[0034] D, cool down, take off the gl...
Embodiment 2
[0036] A kind of rubber glove with antibacterial function, wherein, described rubber latex is made up of following composition, by weight:
[0037]
[0038]
[0039] The antibacterial active ingredient is composed of Luo Han Guo extract and Centella asiatica extract with a weight ratio of 3:4.
[0040] Its preparation method is as follows:
[0041] A, prepare the rubber latex that dipping is used, with natural rubber, emulsified liquid paraffin, colloidal sulfur, zinc oxide, promotor ZDBC, promotor ZMBT, antibacterial active ingredient, fully mix, regulate solid content to be 32%;
[0042] B, after the mold is dried, impregnate the coagulant first, and the coagulant is calcium nitrate or calcium chloride solution of 8% by weight;
[0043] C. Dry the mold, then dip the mold into the rubber latex prepared above, then crimp, then immerse in warm water at 45°C for 2 minutes, take it out, and dry it at high temperature at 120°C for 40 minutes;
[0044] D, cool down, take of...
Embodiment 3
[0046] A kind of rubber glove with antibacterial function, wherein, described rubber latex is made up of following composition, preferably, by weight:
[0047]
[0048] The antibacterial active ingredient is composed of Luo Han Guo extract and Centella asiatica extract with a weight ratio of 2:3.
[0049] Its preparation method is as follows:
[0050] A, prepare the rubber latex that dipping is used, with natural rubber, emulsified liquid paraffin, colloidal sulfur, zinc oxide, promotor ZDBC, promotor ZMBT, antibacterial active ingredient, fully mix, regulate solid content to be 28%;
[0051] B. After the mold is dried, first impregnate the coagulant, which is 10% by weight of calcium nitrate or calcium chloride solution;
[0052] C. Dry the mold, then dip the mold into the rubber latex prepared above, then crimp, then immerse in warm water at 45°C for 2 minutes, take it out, and dry it at a high temperature of 130°C for 30 minutes;
[0053] D, cool down, take off the glo...
PUM
Property | Measurement | Unit |
---|---|---|
elongation | aaaaa | aaaaa |
elongation | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com