Ceramic grinding head material for grinder
A grinding head and grinder technology, applied in the field of kitchen utensils and ceramic materials, can solve the problems of poor chemical corrosion resistance, difficult manufacturing, poor wear resistance and the like
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] In this embodiment, the material of the outer grinding head is composed of 86% of aluminum oxide, 8% of magnesium oxide and 6% of silicon oxide with a purity of ≥99%; the material of the inner grinding head is composed of a purity of ≥99%. 99% alumina 32%, zirconia 53% purity ≥ 94%, magnesia 7% and silicon oxide 8%. The molding pressure used is 430MPa for the outer grinding head and 480MPa for the inner grinding head; the initial firing temperature is 700°C-800°C for the outer grinding head and 550°C-600°C for the inner grinding head; Then the final firing is carried out in two stages. The two stages here mean that the temperature rise process is carried out in two stages, and the final refining temperature is 1675°C-1685°C; the refining uses a hydrogen furnace. This embodiment is the optimal technical solution.
Embodiment 2
[0024] In this embodiment and subsequent embodiments, only the composition of each material and the molding pressure are changed, and the rest are the same as in Embodiment 1.
[0025] The material of the outer grinding head is composed of 80% alumina, 15% magnesium oxide and 5% silicon oxide with a purity of 99% or more; the material of the inner grinding head is composed of 25% alumina with a purity of 99% or more. %, 55% zirconia, 10% magnesia and 10% silicon oxide with a purity of ≥94%. The molding pressure adopted is that the molding pressure of the outer grinding head is 450MPa, and the molding pressure of the inner grinding head is 510MPa.
Embodiment 3
[0027] The material of the outer grinding head is composed of 90% alumina, 5% magnesium oxide and 5% silicon oxide with a purity of 99% or more; the material of the inner grinding head is composed of 45% alumina with a purity of 99% or more. %, Zirconia 45%, Magnesium Oxide 5% and Silicon Oxide 5% with purity ≥94%. The molding pressure adopted is that the molding pressure of the outer grinding head is 450MPa, and the molding pressure of the inner grinding head is 510MPa.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com