Method for manifesting metal surface hidden fingerprints through chemical sedimentation
A metal surface and latent fingerprint technology, which is applied in the field of fingerprint identification, can solve the problems of unrealistic fingerprint detection, fingerprints left for a long time, and limited information extraction, etc., and achieve the effect of clear fingerprint texture details, low cost and high efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0035] A new method for displaying latent fingerprints on more active metal objects. Taking Zn metal objects as an example, for smaller or easy-to-cut objects, the immersion solution method can be used. The specific operation has the following steps:
[0036] 1) Use copper sulfate pentahydrate and ultrapure water as raw materials to prepare copper sulfate mother liquor.
[0037] 2) Weigh 12.484g of copper sulfate pentahydrate with an electronic analytical balance, put it in a 100ml volumetric flask, add ultrapure water to 100ml, and mix well. spare.
[0038] 3) Take the mother solution and dilute it according to the size of the fingerprint object. For sheet metal or thin substrates, how much solution to take is based on: the volume of the mother solution taken / the area of the object = 45μl / ㎝ 2 .
[0039] 4) Object area: 1.0㎝×1.0㎝=1.0㎝ 2 . According to the above formula, the volume of copper sulfate required is about 45μl / ㎝ 2 ×1.0㎝ 2 = 45 μl.
[0040] 5) Take a 10ml c...
Embodiment 2
[0048] Taking the Mg metal object as an example, for small or easy-to-cut objects, the immersion solution method can be used. The specific operation has the following steps:
[0049] 1) Use copper sulfate pentahydrate and ultrapure water as raw materials to prepare copper sulfate mother liquor.
[0050] 2) Weigh 12.484g of copper sulfate pentahydrate with an electronic analytical balance, put it in a 100ml volumetric flask, add ultrapure water to 100ml, and mix well. spare.
[0051] 3) Take the mother solution and dilute it according to the size of the fingerprint object. For sheet metal or thin substrates, how much solution to take is based on: the volume of the mother solution taken / the area of the object = 40μl / ㎝ 2 .
[0052] 4) Object area: 0.9㎝×1.6㎝=1.4㎝ 2 '. According to the above formula, the volume of copper sulfate required is about 40μl / ㎝ 2 ×1.4㎝ 2 =56 μl.
[0053] 5) Take a 10ml clean beaker, add 56μl of the prepared copper sulfate mother solution with a p...
Embodiment 3
[0060] Taking ordinary carbon steel objects as an example, for small or easy-to-cut objects, the immersion solution method can be used. The specific operation has the following steps:
[0061] 1) Use copper sulfate pentahydrate and ultrapure water as raw materials to prepare copper sulfate mother liquor.
[0062] 2) Weigh 12.484g of copper sulfate pentahydrate with an electronic analytical balance, put it in a 100ml volumetric flask, add ultrapure water to 100ml, and mix well. spare.
[0063] 3) Take the mother solution and dilute it according to the size of the fingerprint object. For flake metal or thin substrates, the amount of solution to be taken is based on: the volume of the mother solution taken / the area of the object = 16μl / ㎝ 2 .
[0064] 4) Object area: 2.0㎝×1.5㎝=3.0㎝ 2 '. According to the above formula, the volume of copper sulfate required is about 16μl / ㎝ 2 ×3.0㎝ 2 = 48 μl.
[0065] 5) Take a 10ml clean beaker, add 48μl prepared copper sulfate mother so...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com