Production method of low-carbon environment-friendly anti-deformation solid wood composite door frame
A technology of solid wood composite and production method, which is applied to the jointing of wooden veneers, manufacturing tools, wood processing equipment, etc., can solve the problems of poor nail performance, abnormal color, and non-waterproof, etc., achieve good market application prospects, and solve problems that cannot be solved Environmentally friendly and waterproof, with remarkable cooling effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0047] A method for manufacturing an anti-deformation solid wood composite door edge, as attached figure 1 As shown, the following steps are included: the first step is to cook and peel the logs, then spin them into veneers, and dry them until the moisture content is below 12%;
[0048] In the second step, the surface of the veneer that needs to be bonded is coated with EO-grade environmental protection glue with a mass concentration of 70%, pressed together to form a panel, and the panel is cut into slats of the same specification, and the surface of the slats that need to be bonded is coated with EO-grade environmental protection , the glue whose mass concentration is 70%;
[0049] The third step is to choose three layers of horizontally textured slats, put them in the middle layer of horizontally textured slats, insert the longitudinal textured slats in the middle layer of the three layers of horizontally textured slats, and use a heat press to convert the horizontally text...
Embodiment 2
[0054] The manufacturing method of the anti-deformation solid wood composite door edge described in this embodiment, the first step is to cook and peel the logs, and then use a rotary cutter to cut them into 2mm thick veneers, divide the veneers into three levels, and use the first level veneer On the surface, the second-grade veneer and the third-grade veneer are used in the middle layer, and the first-grade veneer, the second-grade veneer, and the third-grade veneer are dried with a drum or a vacuum dryer to a moisture content of 6-12% .
Embodiment 3
[0056] In the manufacturing method of the anti-deformation solid wood composite door described in this embodiment, in the second step, the surface to be bonded to the veneer is coated with EO grade environmental protection glue with a mass concentration of 70%, and the glue is vegetable glue with zero formaldehyde emission or E0 grade Use melamine glue or phenolic glue to press the veneers coated with glue to form a panel, cut the panel and saw it into slats of the same specification, and coat 100% of the cross-section of the sawed slats with EO High-grade environmental protection glue; the top and bottom panels are glued on the reverse side, and the middle layer strips are double-sided glued.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com