[0010] Embodiment 1, a kind of xonotlite reinforced foam cement is made up of xonotlite slurry of 10-20% by mass and 80-90% of foamed cement, and the solid content of xonotlite slurry is 10%-30%, the balance is composed of water, and the solid content is composed of 50%-60% of Quartz and 4 0%-50% Lime composition, SiO in the quartz used 2 The content is greater than 98%, and the CaO content in the lime used is 90-96%;
[0011] The production method of the above-mentioned xonotlite reinforced foamed cement is to mix the xonotlite slurry with the foamed cement evenly and foam together, and the xonotlite slurry is mixed with a molar ratio of 0.92~1.08 Lime and quartz raw materials are mixed, and water 10 to 30 times the total weight of lime and quartz raw materials is added at the same time, and the calcium silicate active slurry is synthesized by dynamic hydrothermal method. , keep the vapor pressure at 1.8~2.2MPa, react at constant temperature and pressure for 4~8 hours, and...
Embodiment 2
[0013] Embodiment 2, a xonotlite reinforced foamed cement and its production method are based on embodiment 1. In this embodiment, industrial lime and 400 mesh quartz powder are used as calcium and siliceous raw materials. Prepare a slurry with a silicon / silicon molar ratio of 0.92, and a water / solid weight ratio of 10:1. After the prepared slurry is stirred evenly, it is placed in an autoclave with a stirring device, and the temperature is raised to 210°C at a rate of 1.5°C / min. , keep the steam pressure at 1.8~2.2MPa, keep the heat for 4 hours, then stop the heat source for natural cooling, react, and get xonotlite slurry; xonotlite reinforced foam cement is composed of foamed cement and xonotlite slurry according to the formula Proportional composition, that is, first mix the sulphoaluminate cement and ordinary Portland cement in the foamed cement in proportion, then mix with the xonotlite slurry, and then add the foaming agent, reinforcing agent, and polymer to form the fo...
Embodiment 3
[0014] Embodiment 3, a xonotlite reinforced foamed cement and its production method are based on embodiment 1. This embodiment uses industrial lime and 400 mesh quartz powder as calcium and siliceous raw materials. Prepare a slurry with a molar ratio of 1 / silicon, and a water / solid weight ratio of 20:1. After the prepared slurry is stirred evenly, put it into an autoclave with a stirring device, and heat up to 220°C at a rate of 1.5°C / min. , keep the steam pressure at 1.8~2.2MPa, keep it warm for 5 hours, then stop the heat source for natural cooling, react, and get xonotlite slurry; xonotlite reinforced foam cement is composed of foamed cement and xonotlite slurry according to the formula Proportional composition, that is, first mix the sulphoaluminate cement and ordinary Portland cement in the foamed cement in proportion, then mix with the xonotlite slurry, and then add the foaming agent, reinforcing agent, and polymer to form the foamed cement All materials, plant fibers, a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com