Embodiment 1
[0025] Weigh the following raw materials in parts by weight: carbide slag 20-30, fly ash 25-30, cement 5-10, modified nano attapulgite 4-6, water treatment sludge 5-10, alkali slag 5-10, Light calcium powder 5-10, lime 10-15, triethanolamine lime 0.1-0.3% by weight, gypsum 1-3, aluminum powder 0.02-0.08, oxidized paraffin wax soap 3-5% by aluminum powder, bicarbonate Calcium 0.01-0.02, clay residue 2-3, lignocellulose 1-2, water glass 0.3-0.5, sodium hexametaphosphate 1-2, borax 0.03-0.05, hydroxypropyl methylcellulose sodium 1-2, super fine polyvinyl alcohol 1-2,
[0026] Among them, the attapulgite is modified: first soak the attapulgite with 15-20% hydrochloric acid for 1-2 hours, let it stand, clarify, centrifuge, wash the solid with water until it is neutral, and after drying, add an amount equivalent to the weight of the solid 3-5% vinyltriethoxysilane is stirred evenly, dried and ground into nanopowder,
[0027] Process the above-mentioned substances that have been we...
Embodiment 2
[0035] Weigh the following raw materials in parts by weight: calcium carbide slag 25, cement 56, modified nano attapulgite 5, water treatment sludge 8, alkali slag 6, light calcium powder 12, lime 14, 0.1-0.3% of the weight of triethanolamine lime , gypsum 2, aluminum powder 0.05, the amount of oxidized paraffin wax soap is 4% of the weight of aluminum powder, calcium bicarbonate 0.01, white clay slag 3, lignocellulose 1.5, water glass 0.4, sodium hexametaphosphate 1, borax 0.04, hydroxypropyl Sodium methyl cellulose 2, ultrafine polyvinyl alcohol 1, wherein, the modified attapulgite is obtained by the following method: first soak sepiolite with 15% hydrochloric acid for 1-2 hours, let stand, clarify, centrifuge, solid Wash with water until neutral, after drying, add vinyltriethoxysilane equivalent to 3-5% of solid weight, stir evenly, dry, and crush into powder,
[0036] Process the above-mentioned substances that have been weighed into finished aerated bricks according to th...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com