[0016] A kind of softening agent for the production of regenerated rubber, select waste oil as raw material, it comprises the following components by weight percentage: 30% of animal and vegetable oleic acid, 17% of arachidonic acid, 8% of stearic acid, 18% of glycerin; the balance is water and Impurities. Treatment method: first filter the waste oil to remove solid impurities such as mechanical suspended matter contained in it, and then let it stand for 11 hours, the water in the waste oil will deposit to the lower part, and release the water from the lower part, and then heat the waste oil to 200 ° C to make Distill the water remaining in the oil until the water content in the waste oil is less than 0.5%. After cooling down to room temperature, pump the oil into a closed container and heat it to 50-60°C, then vacuumize to remove the odor, and finally add the oil The weight of 5% carbon black is stirred evenly to obtain the softener for the production of regenerated rubber. ...
Embodiment 2
[0022] A kind of softening agent for the production of regenerated rubber, which uses gutter oil as raw material, and comprises the following components in weight percentage: 25% animal and vegetable oleic acid, 15% arachidic acid, 12% stearic acid, and 25% glycerin; the balance is water and Impurities.
[0023] First filter the waste oil to remove solid impurities such as mechanical suspensions contained in it, and then let it stand for 12 hours. The water in the waste oil will deposit to the lower part, and the water will be released from the lower part. Distill the water in the waste oil until the water content in the waste oil is less than 0.5%, remove the odor of the obtained oil by vacuuming, and finally add silicate with an oil weight of 5%, and stir evenly to obtain recycled rubber. softener.
Embodiment 3
[0025] The softening agent used for the production of reclaimed rubber is selected from waste oil raw materials and contains the following components in weight percentage: 20% animal and vegetable oleic acid, 25% arachidonic acid, 15% stearic acid, 15% glycerin; the balance is water and impurities. First filter the waste oil to remove solid impurities such as mechanical suspended matter contained in it, and then let it stand for 10 hours, the water in the waste oil will deposit to the lower part, and the water will be released from the lower part, and then the waste oil will be heated to 180 ° C to make the remaining Distill the water in the waste oil until the water content in the waste oil is less than 0.5%, remove the odor of the obtained oil by vacuuming, and finally add active calcium carbonate with an oil weight of 5%, and stir evenly to obtain regenerated rubber. softener.
PUM
Property | Measurement | Unit |
---|---|---|
breaking strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com