A technology of fire door core board and magnesium chloride solution, which is applied to fire doors and other directions, can solve the problems of fire doors losing fire protection, affecting the overall performance of fire doors, and failing to reach the smoke toxicity index, etc., achieving strong sound absorption and low cost , long service life effect

Inactive Publication Date: 2012-11-14
杨永
View PDF0 Cites 10 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, as far as the current two fire door core panels are concerned, the first one is made of aluminum silicate wool as the main material. Because its smoke toxicity index does not meet the national standard, it has been banned from use; The other is the door core board with expanded perlite as the main material. Due to the poor strength of perlite itself, after bonding with the steel plate or multi-layer board, the processing deformation of the thin steel plate, heat deformation, and collision deformation and other factors , It is easy to cause the core board of the fire door to crack, thus affecting the overall performance of the fire door
After the multi-layer board is bonded with the core board made of perlite, the core board is easily broken by external impact during transportation and installation. In the event of a fire, when the multi-layer board is burned out, the fire door will automatically Falling apart loses its fire protection effect

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment Construction

[0020] Take the following raw material ratio as an example: 100 parts of light-burned magnesium oxide powder, 40 parts of magnesium chloride, 30 parts of water, 0.8 parts of modifier, and 0.3 parts of foaming agent.

[0021] This fire door core board is made by the steps of following sequence:

[0022] A, prepare magnesium chloride solution, magnesium chloride is mixed with water to prepare magnesium chloride solution;

[0023] b. Prepare magnesite slurry, mix magnesium oxide, magnesium chloride solution and modifier uniformly according to technical requirements;

[0024] c, prepare foam, deploy foaming agent into foaming liquid, send into foam with foaming machine;

[0025] d, prepare foamed magnesite cement, mix the prepared magnesite slurry and foam evenly;

[0026] e, forming, pouring the foamed magnesite cement into the pre-prepared mold;

[0027] e, demoulding, after the reaction is solidified, it can be demoulded;

[0028] f. Curing, the board can be used after curi...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
densityaaaaaaaaaa
Login to View More

Abstract

The invention relates to a fireproof plate, in particular to a fireproof door core plate. The invention discloses the energy-saving, environment-protection and light-weight fireproof door core plate with the advantages that the energy is saved, the environment is protected, nontoxicity and harmlessness are realized on human bodies, the fireproof and heat insulation performance is good, the sound absorption effect is good, the intensity is high, the service life is long, and the cost is low. The invention also provides a manufacture method of the door core plate, and the manufacture method has the advantages that the process is simple, and the flow process is short. The fireproof door core plate is made from following materials in parts by mass: 100 parts of magnesium oxide, 40 to 50 parts of magnesium chloride, 30 to 40 parts of water, 0.3 to 1 parts of modifying agents, 0.3 to 0.5 parts of foaming agents and the like.

Description

Technical field: [0001] The invention relates to a fireproof board, in particular to a fireproof door core board. technical background: [0002] As we all know, fire doors made of fire door core panels can save the skeleton support, simplify the production process of fire doors, improve production efficiency, and reduce manufacturing costs. However, as far as the current two fire door core panels are concerned, the first one is made of aluminum silicate wool as the main material. Because its smoke toxicity index does not meet the national standard, it has been banned from use; The other is the door core board with expanded perlite as the main material. Due to the poor strength of perlite itself, after bonding with the steel plate or multi-layer board, the processing deformation of the thin steel plate, heat deformation, and collision deformation and other factors , It is easy to cause the core board of the fire door to crack, thus affecting the overall performance of the fi...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C04B28/32E06B5/16
Inventor 杨永
Owner 杨永
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products