Preparation method of low-viscosity potato octenyl succinic acid starch ester
A technology of octenyl succinic acid and potato starch is applied in the field of preparation of octenyl succinate starch ester, can solve the problems of high viscosity microcapsule wall material and the like of octenyl succinate potato starch ester, and achieves excellent hydrophobicity, The effect of excellent free flow, good stability and thickening
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment approach 1
[0007] Specific embodiment one: the preparation method of low-viscosity potato starch octenyl succinate in the present embodiment is carried out according to the following steps: one, take by weighing potato refined starch, add ultrapure water and stir, potato starch dry base The mass ratio of pure water to pure water is 2:3, then add concentrated hydrochloric acid to make the concentration of HCl in the reaction system 0.78~0.8mol / L, then acidolysis reaction in 45~50℃ constant temperature water bath for 2.5~3h, and then use the mass concentration Adjust the pH value of 1.8%~2% sodium hydroxide solution to 6.50~7.00, then wash with deionized water until no chloride ions appear in the washing liquid, then add ultrapure water and stir well to obtain starch milk, wherein starch milk The dry basis mass content of potato starch in medium is 39%~40%; 2. Under the conditions of 33~35°C and pH value of 7.50±0.05, add octenyl with a mass concentration of 3% to the starch milk dropwise w...
specific Embodiment approach 2
[0009] Specific embodiment two: what this embodiment is different from specific mode one is: the mass concentration of concentrated hydrochloric acid described in step one is 35%~37%. Other steps and parameters are the same as in the first embodiment.
specific Embodiment approach 3
[0010] Embodiment 3: This embodiment differs from Embodiment 1 or Embodiment 2 in that: in step 3, the drying temperature is 50° C., and the drying time is 3-5 hours. Other steps and parameters are the same as those in Embodiment 1 or Embodiment 2.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
degree of substitution | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com