Preparation method for inorganic fire-resistant foam filling material for door core board
A filling material and inorganic foaming technology, which is applied in the field of preparation of fireproof materials, can solve problems such as poor structural stability, poor sound insulation effect, easy deformation and damage, etc., and achieve the effects of increased strength, high foaming effect, and dense pores
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] Weigh 10Kg kaolin, 3Kg coal ash, 55Kg light magnesium chloride, 2.5Kg closed-cell perlite, 15Kg anhydrous magnesium chloride, 5g magnesium sulfate, 2.5Kg animal protein foaming agent, 2Kg K12 foaming agent, 0.5Kg carbon fiber, fireproof bamboo Sign 0.2Kg, water 55Kg to prepare inorganic foam fire-resistant door core board filling material, the steps are as follows:
[0020] (1) Add 15Kg anhydrous magnesium chloride, 5Kg magnesium sulfate, 0.5Kg of carbon fiber, and 0.2Kg of fireproof bamboo sticks into 25Kg of water, stir to form a mixed solution, and make the carbon fiber and fireproof bamboo sticks uniform in the mixed solution;
[0021] (2) 10Kg kaolin, 3Kg coal ash, 55Kg light magnesia, 2.5Kg closed-cell perlite are dropped into the mixed solution of step (1), and stirred into slurry;
[0022] (3) The K12 whipping agent of 2.5Kg animal protein foaming agent, 2Kg is mixed and dropped into 30Kg water, stirs and becomes foaming agent;
[0023] (4) Inject the foaming a...
Embodiment 2
[0025] Weigh 5Kg of kaolin, 6Kg of coal ash, 45Kg of light magnesium oxide, 1.5Kg of closed-cell perlite, 25Kg of anhydrous magnesium chloride, 15Kg of magnesium sulfate, 1.5Kg of animal protein foaming agent, 1Kg of K12 foaming agent, 0.8Kg of carbon fiber, fireproof Bamboo stick 0.3Kg, water 60Kg prepare inorganic foam fireproof door core board filling material, the steps are as follows:
[0026] (1) Add 25Kg of anhydrous magnesium chloride, 15Kg of magnesium sulfate, 0.8Kg of carbon fiber, and 0.3Kg of fireproof bamboo sticks into 35Kg of water, stir to form a mixed solution, and make the carbon fiber and fireproof bamboo sticks uniform in the mixed solution;
[0027] (2) 5Kg kaolin, 6Kg coal ash, 45Kg light magnesia, 1.5Kg closed-cell perlite are dropped into the mixed solution of step (1), and stirred into slurry;
[0028] (3) The K12 whipping agent of 1.5Kg animal protein foaming agent, 1Kg is mixed and dropped into 25Kg water, stirs and becomes foaming agent;
[0029] ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com