A manufacturing method and short fiber technology, applied in the field of chemical polyester fiber manufacturing, can solve the problems of short duration, low luminous brightness, limited application fields, etc., and achieve the effects of long luminous time, stable chemical properties, and high brightness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0011] 1. Preparation of luminescent polyester plastic parts slab and luminescent polyester masterbatch
[0012] Dry the rare earth aluminate luminescent compound and the polyester chips and mix them uniformly with EBS (vinyl bis stearamide) at a ratio of 15-20% by weight: 78.5-84%: 1-1.5%, and then pass through a twin-screw Blending, melting, extruding, and cooling with water to prepare 15-20% light-emitting polyester plastic parts slab and light-emitting polyester masterbatch.
[0013] 2. Manufacture of luminous polyester staple fiber
[0014] The luminescent polyester masterbatch and polyester chips are uniformly mixed at a ratio of 20%:80%, melted, extruded, and metered through a screw spinning machine, and then enter the spinning box and spinning assembly, and then cooled and oiled by the surrounding air. , winding, balancing, bundling, oil bath heating, drawing, crimping, relaxation heat setting, cutting, packing, to obtain luminescent polyester staple fibers containing...
Embodiment 2
[0023] 1. Preparation of luminescent polyester plastic parts slab and luminescent polyester masterbatch
[0024] Dry the rare earth aluminate luminescent compound and the polyester chips and mix them uniformly with EBS (vinyl bis stearamide) at a ratio of 20-30% by weight: 68-78.5%: 1.5-2%, and then pass through a twin-screw Blending, melting, extruding, and cooling with water to prepare 20-30% light-emitting polyester plastic parts slab and light-emitting polyester masterbatch.
[0025] 2. Manufacture of luminous polyester staple fiber
[0026] The luminescent polyester masterbatch and polyester chips are evenly mixed at a ratio of 22%:78%, melted, extruded, and metered through a screw spinning machine, and then enter the spinning box and spinning assembly, and then cooled and oiled by the surrounding air. , winding, balancing, bundling, oil bath heating, drawing, crimping, relaxing heat setting, cutting, and packaging to obtain luminous polyester staple fibers containing 4....
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com