Lightweight brick with mullite roll bar waste as raw material and preparation method thereof
A technology for mullite and lightweight bricks, which is applied in the field of lightweight bricks and its preparation, can solve problems such as the inability to guarantee the uniformity of pores, instability, and the limited scope of application of porous material methods, so as to promote environmental protection and sustainable development, The effect of reducing the temperature drop rate of molten steel and reducing solid pollution
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A lightweight brick using mullite roller waste as raw material and a preparation method thereof. Firstly, 50-60wt% mullite roller waste, 28-40wt% clay clinker, 0.1-3wt% α-Al 2 o 3 Micropowder, 0.1~2wt% ρ-Al 2 o 3 Micropowder, 3-5wt% of nano silicon dioxide and 6-9wt% of kyanite powder are mixed, plus 20-30wt% of water and 0.1-0.2wt% of sodium hexametaphosphate, mixed for 3-8 minutes to prepare Slurry and foam made by adding 0.1-0.2wt% foaming agent, mix evenly, pour into molding, dry at room temperature for 4-10 hours, and then dry at 100-110°C for 3-5 hours After demoulding, it is finally fired at 1350-1400°C and kept warm for 3-5 hours.
[0017] The bulk density of the mullite lightweight bricks prepared in Example 1 is 0.75 to 0.80 g / cm 3 , the thermal conductivity is 0.25~0.3w / (m.k), the compressive strength reaches 6.0~6.8MPa, and the reburning line change is 0.9~1.0%.
Embodiment 2
[0019] A lightweight brick made of mullite roller waste as a raw material and a preparation method thereof. First, 60-68wt% of mullite roller bar waste, 19-28wt% of clay clinker, 3-6wt% of α-Al 2 o 3 Micropowder, 2~4wt% ρ-Al 2 o 3 Mix micropowder, 2-3wt% silicon micropowder and 4-6wt% kyanite micropowder, add 30-40wt% water and 0.2-0.3wt% sodium tripolyphosphate, mix for 8-15 minutes, and prepare a slurry , and then add 0.2-0.3wt% foaming agent to make the foam, mix it evenly, cast it, dry it at room temperature for 10-16 hours, and then dry it at 110-120°C for 5-7 hours to release the mold. Finally, it is fired under the condition of 1400-1450°C and kept for 5-7 hours.
[0020] The bulk density of the mullite lightweight bricks prepared in Example 2 is 0.74~0.76g / cm 3 , the thermal conductivity is 0.24~0.28w / (m.k), the compressive strength reaches 5.8~6.2MPa, and the reburning line change is 0.98~1.0%.
Embodiment 3
[0022] A lightweight brick made of mullite roller waste as a raw material and a preparation method thereof. First, 68-74wt% of mullite roller bar waste, 15-19wt% of clay clinker, 6-8wt% of α-Al 2 o 3 Micropowder, 4~6wt% ρ-Al 2 o 3 Mix micropowder, 0.1-2wt% silicon micropowder and 0.1-4wt% kyanite micropowder, add 10-20wt% water and 0.2-0.3wt% sodium lignosulfonate, mix for 3-8 minutes, and prepare the material Slurry, and then add 0.1-0.2wt% foaming agent to make foam, mix evenly, pour into molding, dry at room temperature for 16-20 hours, and then dry at 100-110°C for 7-10 hours to release the mold , and finally fired at 1450-1500°C and kept for 7-12 hours.
[0023] The bulk density of the mullite lightweight bricks prepared in Example 3 is 0.78~0.82g / cm 3 , the thermal conductivity is 0.26~0.3w / (m.k), the compressive strength reaches 6.3~6.8MPa, and the reburning line change is 0.9~1.0%.
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
strength | aaaaa | aaaaa |
density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com