Preparation method of waterproof fluorescent powder
A fluorescent powder and waterproof technology, applied in chemical instruments and methods, luminescent materials, etc., can solve the problems of poor luminous performance of coated phosphors, loss of performance of long-lasting phosphors, poor weather resistance of phosphors, etc., and achieve low overall cost , Improve water resistance and avoid performance degradation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] Weigh 20 grams of aluminate long-lasting phosphor, and prepare a phosphor suspension with a concentration of 2g / 100ml with ethylene glycol; weigh NaSiO 3 9H 2 O 1 g, added to the phosphor suspension, stirred while ultrasonically dispersed for 30 min. The suspension was heated to 80°C and maintained while stirring. Prepared HNO 3 A solution with a volume ratio of 1:100 to absolute ethanol is added dropwise to the phosphor suspension at a rate of 2ml / min, and the pH meter display value of the phosphor suspension is controlled to be 10, and the dripping is stopped. Continue to keep warm and stir for 4 hours, centrifuge the suspension, wash it twice with absolute ethanol, and fully dry it in an oven. The coated phosphor is baked at 300°C for 1 hour, and the surface-coated SiO can be obtained after cooling. 2 aluminate phosphors.
Embodiment 2
[0026] Weigh 20 grams of aluminate long-lasting phosphor, and prepare a phosphor suspension with a concentration of 2g / 100ml with ethylene glycol; weigh NaSiO 3 9H 2 O 1 g, added to the phosphor suspension, stirred while ultrasonically dispersed for 30 min. The suspension was heated to 90°C and maintained while stirring. All the other conditions are with embodiment 1.
Embodiment 3
[0028] Weigh 20 grams of aluminate long-lasting phosphor, and prepare a phosphor suspension with a concentration of 2g / 100ml with ethylene glycol; weigh NaSiO 3 9H 2 O 1 g, added to the phosphor suspension, stirred while ultrasonically dispersed for 30 min. The suspension was heated to 80°C and maintained while stirring. Prepared HNO 3 A solution with a volume ratio of 1:100 to absolute ethanol was added dropwise into the phosphor suspension at a rate of 2ml / min, and the display value of the pH meter of the phosphor suspension was adjusted to 10.5. All the other conditions are with embodiment 1.
PUM
![No PUM](https://static-eureka-patsnap-com.libproxy1.nus.edu.sg/ssr/23.2.0/_nuxt/noPUMSmall.5c5f49c7.png)
Abstract
Description
Claims
Application Information
![application no application](https://static-eureka-patsnap-com.libproxy1.nus.edu.sg/ssr/23.2.0/_nuxt/application.06fe782c.png)
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com