A technology for controlled-release tablets and oxycodone, which is applied in the directions of pill delivery, organic active ingredients, non-active ingredients of polymer compounds, etc., can solve problems such as adverse reactions, coagulation disorders in the gastrointestinal tract, etc. Simple, high-quality effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0039] Embodiment 1: specification 1000 pieces
[0040] prescription:
[0041] Oxycodone 5 / 10 / 20 / 40g
[0042] Dextrin 300g
[0043]Polyethylene 300g
[0044] 70% pvp ethanol solution appropriate amount
[0045] Prescription of coating solution
[0046] Cellulose acetate 50g
[0047] Polysorbate-80 appropriate amount
[0048] Dibutyl phthalate Appropriate amount
[0049] Add 90% ethanol-acetone solution to 1000ml
[0050] Preparation method:
[0051] The oxycodone, dextrin and polyethylene are mixed evenly, granulated with 70% pvp ethanol solution, dried, granulated and compressed into tablets. Take cellulose acetate, appropriate amount of polysorbate-80, appropriate amount of dibutyl phthalate, dissolve with 1000ml of 90% ethanol-acetone mixed solvent to prepare coating solution. Coating until the weight of each coating layer is 8.5-9mg. Finished product inspection, coating.
Embodiment 2
[0052] Embodiment 2: specification 10000 pieces
[0053] prescription:
[0054] Oxycodone 400g
[0055] Dextrin 3000g
[0056] Polyethylene 3000g
[0057] 70% pvp ethanol solution appropriate amount
[0058] Prescription of coating solution
[0059] Cellulose acetate 500g
[0060] Polysorbate-80 amount
[0061] Dibutyl phthalate Appropriate amount
[0062] Add 90% ethanol-acetone solution to 10000ml
[0063] Preparation method:
[0064] The oxycodone, dextrin and polyethylene are mixed evenly, granulated with 70% pvp ethanol solution, dried, granulated and compressed into tablets. Take cellulose acetate, appropriate amount of polysorbate-80, appropriate amount of dibutyl phthalate, dissolve with 1000ml of 90% ethanol-acetone mixed solvent to prepare coating solution. Coating until the weight of each coating layer is 8.5-9mg. Finished product inspection, coating.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com