Wood wax oil for protecting lumber and preparation technique thereof
A technology of wood wax oil and wood, which is applied to wood processing equipment, impregnated wood, and manufacturing tools, etc., can solve the problems of simple termite control and flame retardant treatment, and achieve the effects of preventing dry cracking, eliminating incorporation, and simple preparation process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] Embodiment 1 gets each raw material by following weight parts:
[0027] 54 parts of linseed oil, 35 parts of tung oil, 10 parts of crude beeswax, 1 part of iron oxide, 0.01 part of catalyst,
[0028] Heat linseed oil and tung oil together at 250-290°C for 10-12 hours, react to the end and then when the temperature drops to 80-90°C, disperse and add the wax at high speed, then add inorganic pigments and rare earth drier, stir and mix evenly , to obtain the wood wax oil.
[0029] The wood wax oil for wood protection can be directly used for spray protection of wood products, and can also be used for infiltration of molded products after dilution with environmentally friendly organic solvents. After testing, the treated wood products will not produce any toxic and harmful substances. At the same time, it can meet the excellent performance of breathability, waterproof, moisture-proof, insect-proof, anti-corrosion and crack-proof.
Embodiment 2
[0030] Embodiment 2 gets each raw material by following weight parts:
[0031] 60 parts of sunflower oil, 25 parts of tung oil, 10 parts of carnauba wax, 5 parts of iron oxide, 0.1 part of catalyst, heat sunflower oil and tung oil at 250-290 ° C for 10-12 hours, react to the end and then the temperature drops to 80 At -90°C, disperse and add wax at high speed, then add inorganic pigment and rare earth drier, stir and mix evenly to obtain the wood wax oil.
Embodiment 3
[0032] Embodiment 3 gets each raw material by following weight parts:
[0033] 60 parts of soybean oil, 15 parts of carnauba wax, 1 part of iron oxide, 0.1 part of catalyst, 0.3 part of commercially available modified silicone oil dispersant, 0.01 part of dimethyl silicone oil defoamer,
[0034] Heat and melt carnauba wax, then filter to obtain refined carnauba wax, then add soybean oil and catalyst, stir and react for 40 minutes under temperature control conditions of 180-250°C, then add iron oxide, commercially available modified silicone oil dispersant and Simethicone defoamer, stirred until evenly mixed to obtain the wood wax oil in paste form.
PUM
Property | Measurement | Unit |
---|---|---|
melting point | aaaaa | aaaaa |
melting point | aaaaa | aaaaa |
refractive index | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com