Aging method after dying of all-cotton knitting clothes
A garment dyeing and cotton knitting technology, applied in the directions of dyeing, fiber treatment, physical treatment, etc., can solve the problems of old cotton knitted garments being washed, and achieve the effect of good air permeability and good elasticity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] A) Finish the finished garment after dyeing. Specifically, make sure that the front and back of the finished garment are distinguished before being sent to the stone mill. Make sure that the front is facing outwards. The curling part needs to be ironed and flattened. Check whether the bag cover is sewn or not. Garments with plackets should be temporarily stitched with threads. For garments without flaps and / or plackets, the corresponding sewing operations can be omitted to obtain the garments to be ground;
[0024] B) Select pumice stone, preferably 1.8-2.2×1.8-2.2×3.8-4.2cm pumice made in Indonesia. Pumice with a specific gravity of <1 should account for 9-11%, and the Mohs hardness should be controlled to <2, and The selected part of the pumice is pre-soaked in a container such as a tank, vat, or barrel containing a potassium permanganate solution with a concentration of 0.08% for 25-35 minutes, and then taken out and drained for 10-20 minutes to obtain an impregnated pot...
Embodiment 2
[0028] Change the strong oxidant solution in step B) to a sodium hypochlorite solution with a concentration of 1%; in step C), the volume ratio of dry and wet pumice in the chamber of the stone mill is 40:1, that is, dry and wet pumice The occupancy rate is 40%, and the stone grinding time is 12min; in step D), the clean water is heated to 60℃, and 3g / L of soda is added to clean for 9min. The amount of soda ash is 0.9g / L, softener, fluffing agent, silicone oil for cotton The added amount is 9%, 2.2%, 1.2% of the weight of the garment. The garment is dehydrated to a moisture content of 28%, and cold air is introduced for 26 minutes. The rest is the same as described in Example 1.
Embodiment 3
[0030] Change the concentration of the potassium permanganate solution in step B) to 2%; the volume ratio of dry and wet pumice in step C) in the chamber of the stone mill is 35:1, that is, dry and wet pumice The occupancy rate is 35%, the stone grinding time is 8min; the clean water in step D) is heated to 65℃, and 4g / L oxalic acid is added for cleaning for 10min, the soda ash content is 1g / L, cotton softener, fluffing agent, silicone oil The added amount is 8.5%, 2.5%, 1.5% of the weight of the garment. The garment is dehydrated to a moisture content of 27%, and cold air is introduced for 27 minutes. The rest are the same as those described in Example 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com