A polyvinyl chloride and calendering film technology, which is applied in the field of plastic film production, can solve the problems of uneven film thickness, red blood cell damage, damage, etc., achieve the effects of smooth inner and outer surfaces, increase blood storage time, and improve storage quality
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] Embodiment 1 of the present invention: Various devices of the present invention can be assembled using finished products in the existing market, wherein the extruder adopts a six-stage extruder, and the calender adopts a four-roll calender. During processing, the powdery polyvinyl chloride material is added to the high-speed mixer and kneaded at a high speed. After full mixing and preliminary plasticization, it is sent to the six-stage extruder for uniform extrusion. The temperature of each stage of the six-stage extruder is set as: 129°C~133°C, 121°C~135°C, 141°C~145°C, 141°C~145°C, 143°C~147°C, 143°C~147°C; the best set temperature is: 131°C, 133°C, 143°C °C, 143 °C, 145 °C, 145 °C. The extruded material is sent into the melting machine to carry out rubber mixing on the material, and the low molecular substances are volatilized. The temperature of mastication is 165℃~175℃. Then, after filtering in a filter with a temperature of 170°C to 175°C, it is calendered and f...
Embodiment 2
[0014] Embodiment 2 of the present invention: Add the granular polyvinyl chloride material into a high-speed mixer and knead at a high speed. After fully mixing and preliminary plasticization, it is sent into a six-stage extruder for uniform extrusion. Segment temperature settings: 114°C to 118°C, 116°C to 120°C, 126°C to 130°C, 126°C to 130°C, 128°C to 132°C, 128°C to 132°C; the best set temperature for each segment For: 116°C, 118°C, 128°C, 128°C, 130°C, 130°C. The extruded material is sent into the melting machine to carry out rubber mixing on the material, and the low molecular substances are volatilized. The temperature of rubber mixing is set at 160°C to 170°C. Then filter in a filter at a temperature of 165°C to 170°C, and then calender and form through a four-roller calender. The temperature of the four rollers is set as: 182°C to 184°C, 182°C to 184°C, and 183°C ~185℃, 179℃~181℃; the temperature of the 4 rollers is best set as: 183℃, 183℃, 184℃, 180℃. Then the film...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com