Embodiment 1
[0019] Add 5 g of sodium tetraborate (Na 2 B 4 o 7 ), 0.01 g of sodium dodecylbenzenesulfonate (C 18 h 29 SO 3 Na) and 10 grams of mannitol (C 6 h 14 o 6 ), prepared 1 liter of solution, and stirred for 5 hours to obtain an anti-pollution coating composition.
Embodiment 2 and 3
[0021] The process of Example 1 was repeated to obtain two antipollution coating compositions containing 15 grams and 20 grams of mannitol respectively.
Embodiment 4
[0023] 1 g of sodium tetraborate, 0.01 g of sodium dodecylbenzenesulfonate, and 1 g of mannitol were added to distilled water to prepare 1 liter of a solution, and stirred for 5 hours to obtain an anti-pollution coating composition. Comparative example 1
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com