Casing of electronic device
A technology for electronic devices and housings, which is applied to electrical equipment housings/cabinets/drawers, devices for coating liquid on the surface, electrolytic coatings, etc., and can solve problems such as corrosion of dirt, single color of metal layers, and poor decorative effects , to achieve the effect of strong corrosion resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
no. 1 example
[0018] The first embodiment: the above-mentioned polished shell is chemically degreased, then washed with water, then chemically treated, washed with water again, and then the pretreated shell is placed in a tank filled with electrolyte and passed through The treatment is carried out in an electrolytic cell with direct current. In this embodiment, the above-mentioned electrolyte is a mixed solution of sulfuric acid and sulfosalicylic acid (Sulfosalicylic Acid), wherein the weight percent concentration of the sulfuric acid is 0.1-1%, and the weight of the sulfosalicylic acid (Sulfosalicylic Acid) is The percentage concentration is 10-20%. The DC voltage is 40-80V, the current density is 1-4A / dm2, and the treatment time is 15 minutes to 1 hour, until a layer of colored oxide film with a thickness of 3-30 μm is formed on the surface of the shell. Finally, sealing treatment (Sealing Treatment) is performed on the shell with the oxide film on the surface.
no. 2 example
[0019] The second embodiment: degrease the above-mentioned polished casing, then wash it with water, then perform electrolysis or chemical polishing, and wash it with water again, then put the pretreated casing into a tank filled with electrolyte and pass through Anodizing is carried out in an electrolytic bath with direct current. In this embodiment, the above electrolyte is sulfuric acid with a concentration of 150-20000 g / L. The above DC voltage is 12-20V, and the current density is 1-2A / dm 2 , the treatment time is 15 minutes to 1 hour, until the thickness of the oxide film reaches 3-30 μm. Finally, the shell with the oxide film on the surface is sealed.
[0020] In the second embodiment, the anodized casing can be colored before the sealing treatment so that the surface of the casing can obtain the desired color or pattern, wherein the coloring treatment can use adsorption coloring or electrolytic coloring for coloring.
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
surface roughness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com