A technology of siloxane gel and composition, which is applied in the direction of mechanical equipment, other chemical processes, low internal friction springs, etc., can solve the problems that it is impossible to obtain high vibration-absorbing performance gel, and achieve the effect of excellent vibration-absorbing performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment
[0034] To 2000 g of silanol-terminated polydimethylsiloxane (molecular weight 10,000) was added 16.3 g of aminopropyldimethoxysilane. This mixture was stirred and reacted at 100° C. for 2 hours by nitrogen substitution. Thereafter, excess aminopropyltrimethoxysilane was removed by vacuum suction, thereby obtaining polydimethylsiloxane having a viscosity of 10000 cps and one end blocked by an amino group. To 100 g of the obtained resin was added 0.77 g of 2-isocyanatoethyl methacrylate. The mixture was stirred at 50° C. with nitrogen substitution and reacted for 1 hour, thereby obtaining (A) as component (a).
[0035] 50-cSt dimethylpolysiloxane (TMDMS) having a trimethylsilyl group at the end was added in the amount shown in Table 1 as component (b).
[0036] Fumed silica (Aerosil 200, manufactured by Nippon Aerosil Co., Ltd.) was added in the amount shown in Table 1 as component (c).
[0037] Amorphous powder of a three-dimensionally crosslinked silicone resin (Trefil R-90...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com