A technology for leak detection agent and gas, applied in the field of gas leak detection agent and its preparation, can solve the problems of large bubble diameter, easy residue, inaccurate location of leak points, etc., and achieves suitable bubble diameter, small residual and good traceability. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0034] A gas leak detection agent, comprising component A, component B, and component C, and the mass ratio of component A to component B and component C is 39:47:35;
[0035] Component A includes the following components in parts by weight: 30 parts of deionized water, 1 part of n-heptanoic acid, 1 part of dodecanedioic acid, 6.5 parts of triethanolamine, 0.3 part of borate ester, and 0.2 part of benzotriazole ;
[0036] Component B comprises the following components by weight: 45 parts of deionized water, 0.49 part of cocoic acid diethanolamide, 0.07 part of poloxamer 407, and 1.44 part of propylene glycol;
[0037] Component C includes the following components by weight: 30 parts of deionized water, 0.1 part of guar gum, 0.1 part of sodium metasilicate pentahydrate, and 4.8 parts of glycerin;
[0038] Its preparation method comprises the following steps:
[0039] S1. Prepare each component according to the formula of the following gas leak detector:
[0040] S2. Mix the ...
Embodiment 2
[0045] A gas leak detection agent, comprising component A, component B, and component C, and the mass ratio of component A to component B and component C is 68:63:48;
[0046] Component A includes the following components in parts by weight: 45 parts of deionized water, 3 parts of n-heptanoic acid, 3 parts of dodecanedioic acid, 16 parts of triethanolamine, 0.5 part of borate ester, and 0.5 part of benzotriazole ;
[0047] Component B includes the following components by weight: 60 parts of deionized water, 0.9 part of cocoic acid diethanolamide, 0.1 part of Poloxamer 407, and 2 parts of propylene glycol;
[0048] Component C includes the following components by weight: 40 parts of deionized water, 0.5 part of guar gum, 0.5 part of sodium metasilicate pentahydrate, and 7.0 parts of glycerin;
[0049] Its preparation method comprises the following steps:
[0050] S1. Prepare each component according to the formula of the following gas leak detector:
[0051] S2. Mix the deio...
Embodiment 3
[0056] A gas leak detection agent, comprising component A, component B, and component C, and the mass ratio of component A to component B and component C is 50:52.5:41;
[0057] Component A includes the following components in parts by weight: 35 parts of deionized water, 2 parts of n-heptanoic acid, 2 parts of dodecanedioic acid, 10.3 parts of triethanolamine, 0.4 parts of borate esters, and 0.3 parts of benzotriazole ;
[0058] Component B includes the following components by weight: 50 parts of deionized water, 0.63 part of cocoic acid diethanolamide, 0.09 part of Poloxamer 407, and 1.78 part of propylene glycol;
[0059] Component C includes the following components by weight: 35 parts of deionized water, 0.25 parts of guar gum, 0.25 parts of sodium metasilicate pentahydrate, and 5.5 parts of glycerin;
[0060] Its preparation method comprises the following steps:
[0061] S1. Prepare each component according to the formula of the following gas leak detector:
[0062] S...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com