Embodiment 1
[0020] Embodiment 1: The oil-based spacer fluid for well cementing and cementing, the raw materials include 20 to 160 parts of weighting material, 10 to 20 parts of wetting agent, 5 to 22 parts of organic soil, and 50 parts of oil in terms of parts by weight. to 95 parts, 2 to 8 parts of suspending agent, 2 to 5 parts of dispersant, 5 to 6 parts of polymer fluid loss reducer, 10 to 25 parts of emulsifier and 6 to 21 parts of water, according to the following The above steps are obtained: in the first step, the required amount of water is added to the reactor; in the second step, the required amount of suspending agent is added to the water, and the first mixture is obtained after stirring and reacting at a speed of 3800rpm to 4200rpm for 8min to 10min ; The third step is to add the required amount of oil, dispersant, polymer fluid loss reducer and emulsifier to the first mixture in turn, and stir the reaction at a speed of 3800rpm to 4200rpm for 8min to 10min, then increase the...
Embodiment 2
[0022] Embodiment 2: The oil-based spacer fluid for cementing and cementing, the raw materials include 20 or 160 parts of weighting material, 10 or 20 parts of wetting agent, 5 or 22 parts of organic soil, and 50 parts of oil in terms of parts by weight. or 95 parts, 8 or 8 parts of suspending agent, 2 or 5 parts of dispersant, 5 or 6 parts of polymer fluid loss reducer, 10 or 25 parts of emulsifier and 6 or 21 parts of water, according to the following The above steps are obtained: the first step, the required amount of water is added to the reactor; the second step, the required amount of suspending agent is added to the water, and the first mixture is obtained after stirring and reacting at a speed of 3800rpm or 4200rpm for 8min or 10min ; The third step is to add the required amount of oil, dispersant, polymer fluid loss reducer and emulsifier to the first mixture in turn, and stir the reaction at a speed of 3800rpm or 4200rpm for 8min or 10min, then increase the speed to 9...
Embodiment 3
[0023] Embodiment 3: As an optimization of the above embodiment, the weighting material is at least one of iron ore powder, barite and chromium-manganese powder. The inertness of the weighting material prevents it from participating in the reaction of the slurry, and the low content of the weight enables it to disperse evenly and reduce the thixotropy of the slurry.
PUM
Property | Measurement | Unit |
---|---|---|
density | aaaaa | aaaaa |
density | aaaaa | aaaaa |
density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com