Metal bridge structure with shadow elimination effect and touch screen comprising metal bridge structure
A metal bridge and touch screen technology, which is applied in the field of metal bridge structures and touch screens, can solve problems such as brightness, obvious bridge points, and narrow application range
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0035] Such as Figure 4 As shown, a metal bridge structure with shadow elimination effect, the structure includes three folding lines 1, two adjacent folding lines are connected end to end to form two bending parts, and have two free ends, the free ends are respectively connected From the electrodes 2 at both ends of the metal bridge structure, the shape of the entire metal bridge resembles a "Z" shape when viewed from above. The metal bridge includes CuNi / Cu / CuNiTi three-layer stacked metal film layer, the surface metal film layer is blackened, the reflectivity is below 35%, the surface resistance is 0.6Ω, and the width of the metal bridge is 10 μm.
[0036] The preparation of the metal bridge structure with shadow elimination effect specifically includes the following steps:
[0037] 1) CuNi / Cu / CuNiTi three-layer metal film is sequentially plated on the surface of the product that needs to be equipped with a metal bridge structure by magnetron sputtering. When magnetron sp...
Embodiment 2
[0040] Embodiment 2: as Figure 5 As shown, a metal bridge structure with shadow elimination effect, the structure includes 5 fold lines, the end-to-end connection between two adjacent fold lines forms a total of 4 bending parts, and has two free ends, the free ends are respectively connected to Electrodes at both ends of the metal bridge structure. The metal bridge includes a metal film layer stacked in three layers of MoAlMo, the surface metal film layer is blackened, the reflectivity is 30%, the surface resistance is 0.4 ohm, and the width of the metal bridge is 10 μm. The preparation method is the same as that in Example 1. When magnetron sputtering the Mo metal film, a certain amount of nitrogen is filled in the sputtering gas, wherein the volume ratio of nitrogen to the sputtering gas is 25%.
Embodiment 3
[0041] Embodiment 3: A metal bridge structure with shadow elimination effect, the structure includes 4 fold lines, the end-to-end connection between two adjacent fold lines forms 3 bending parts in total, and has two free ends, the free ends are respectively connected to the electrodes at both ends of the metal bridge structure. The metal bridge includes a CuNi / Cu / CuNi three-layer stacked metal film layer, the surface metal film layer is blackened, the reflectivity is 35%, the surface resistance is 0.6 ohm, and the metal bridge width is 15 μm. The preparation method is the same as that in Example 1. A certain amount of oxygen is filled in the sputtering gas when the CuNi metal film is magnetron sputtered, and the volume ratio of nitrogen to the sputtering gas is 10%.
PUM
Property | Measurement | Unit |
---|---|---|
angle | aaaaa | aaaaa |
width | aaaaa | aaaaa |
width | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com