Nanosilver disinfection antibacterial air filter element and preparation method thereof
An air filter, nano-silver technology, applied in botany equipment and methods, disinfectants, separation methods, etc., can solve problems that affect the use of air filters, air filter mildew, fragile equipment, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0035] In the present embodiment, the preparation method of the above-mentioned nano-silver disinfection and antibacterial air filter comprises the following steps:
[0036] S1: Preparation of nano-silver disinfection and antibacterial non-woven fabric 10 in the hydrophobic layer, see Table 1 and Table 2 for details, as follows:
[0037] S11: The preparation of disinfecting and antibacterial nano-silver-silver ion solution, according to parts by weight, including:
[0038]
[0039] S12: Take a suitable hydrophobic non-woven fabric as a carrier, soak the hydrophobic non-woven fabric carrier in the above-mentioned disinfected and antibacterial nano-silver-silver ion solution for 10-30min according to the mass ratio of 1:50-1000;
[0040] S13: Take out the hydrophobic non-woven fabric carrier in the sterilized antibacterial nano-silver-silver ion solution, and dry it at 80-120°C for 10-30min;
[0041] S14: Take out the non-woven fabric after drying, and prepare the nano-silve...
Embodiment 1
[0053] In the present embodiment, the preparation method of the above-mentioned nano-silver disinfection and antibacterial air filter comprises the following steps:
[0054] S1: Preparation of nano-silver disinfection and antibacterial non-woven fabric 10 in the hydrophobic layer, see Table 1 and Table 2 for details, as follows:
[0055] S11: The preparation of disinfecting and antibacterial nano-silver-silver ion solution, according to parts by weight, including:
[0056]
[0057] S12: Take a suitable hydrophobic non-woven fabric as a carrier, and soak the hydrophobic non-woven fabric carrier in the above-mentioned disinfected and antibacterial nano-silver-silver ion solution for 10-30 minutes at a mass ratio of 1:50;
[0058] S13: Take out the hydrophobic non-woven fabric carrier in the sterilized antibacterial nano-silver-silver ion solution, and dry it at 80-120°C for 10-30min;
[0059] S14: Take out the non-woven fabric after drying, and prepare the nano-silver disinf...
Embodiment 2
[0070] In the present embodiment, the preparation method of the above-mentioned nano-silver disinfection and antibacterial air filter comprises the following steps:
[0071] S1: Preparation of nano-silver disinfection and antibacterial non-woven fabric 10 in the hydrophobic layer, see Table 1 and Table 2 for details, as follows:
[0072] S11: The preparation of disinfecting and antibacterial nano-silver-silver ion solution, according to parts by weight, including:
[0073]
[0074] S12: Take a suitable hydrophobic non-woven fabric as a carrier, and soak the hydrophobic non-woven fabric carrier in the above-mentioned disinfected antibacterial nano-silver-silver ion solution for 10-30 minutes according to the mass ratio of 1:200;
[0075] S13: Take out the hydrophobic non-woven fabric carrier in the sterilized antibacterial nano-silver-silver ion solution, and dry it at 80-120°C for 10-30min;
[0076] S14: Take out the non-woven fabric after drying, and prepare the nano-silv...
PUM
Property | Measurement | Unit |
---|---|---|
radius | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com