Environment-friendly nail-free glue special for advertising words and preparation method thereof
A technology of advertising characters and nail-free glue, which is applied in the direction of adhesives, adhesive types, mineral oil hydrocarbon copolymer adhesives, etc., can solve the problems of opaque colloids and cannot meet the needs of transparent products, so as to ensure transparency and improve Transparency durability, effect of increasing viscosity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0034] The composition ratio of a special nail-free glue for environmental protection advertising characters:
[0035]
[0036] What the linear SBS rubber of this embodiment adopts is SBS rubber C501H, and what the star-shaped SBS rubber adopts is SBS rubber C711.
[0037] What the modified castor oil of the present embodiment adopts is MT-ST (commercially available product).
[0038] The preparation method is as follows:
[0039] a. Put 6# solvent oil and methyl acetate into the high-speed dispersing dynamic mixer in turn, start stirring, and add C501H, C711, hydrogenated rosin resin, hydrogenated C9 resin, hydrogenated C5 resin, polyα-methylstyrene resin and SBS resin, stir for 2 to 3 hours until the material is evenly dispersed.
[0040] b. Add fumed silica, MT-ST and antioxidant T501 in sequence, and stir for 10-30 minutes at a speed of 1000±50r / min until the materials are evenly dispersed, and the special nail-free glue for environmental protection advertising charac...
Embodiment 2
[0042] The composition ratio of a special nail-free glue for environmental protection advertising characters:
[0043]
[0044]
[0045] What the linear SBS rubber of this embodiment adopts is SBS rubber C501H, and what the star-shaped SBS rubber adopts is SBS rubber C711.
[0046] The modified polyamide wax powder used in this embodiment is MT-PLUS (commercially available product).
[0047] The preparation method is as follows:
[0048] a. Put cyclohexane and methyl acetate into the high-speed dispersing dynamic mixer in turn, start stirring, add C501H, C711, hydrogenated rosin resin, hydrogenated C5 resin, poly-α-methylstyrene resin and SBS resin in turn, and stir for 2 ~3 hours until the material is evenly dispersed.
[0049] b. Add fumed silica, MT-PLUS and antioxidant T501 in sequence, and stir for 10-30 minutes at a speed of 1000±50r / min until the materials are evenly dispersed, and the special nail-free glue for environmental protection advertising characters is...
Embodiment 3
[0051] The composition ratio of a special nail-free glue for environmental protection advertising characters:
[0052]
[0053]
[0054] What the linear SBS rubber of this embodiment adopts is SBS rubber C501H, and what the star-shaped SBS rubber adopts is SBS rubber C711.
[0055] What the modified castor oil of the present embodiment adopts is MT-ST (commercially available product).
[0056] The preparation method is as follows:
[0057] a. Put cyclohexane and methyl acetate into the high-speed dispersing dynamic mixer in turn, start stirring, add C501H, C711, hydrogenated rosin resin, poly-α-methylstyrene resin and SBS resin in turn, and stir for 2 to 3 hours to The material is dispersed evenly.
[0058] b. Add fumed silica, MT-ST and antioxidant T501 in sequence, and stir for 10-30 minutes at a speed of 1000±50r / min until the materials are evenly dispersed, and the special nail-free glue for environmental protection advertising characters is prepared.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com