A kind of ES fiber containing wormwood extract and preparation method thereof

A technology of extract and wormwood, which is applied in the field of ES fiber containing wormwood extract and its preparation, can solve the problems of reducing functionality, adding unnatural antibacterial ingredients, loss, etc., to achieve good water absorption of fabrics and long-lasting antibacterial Good sex, reduce loss effect

Active Publication Date: 2021-05-18
BESTEE MATERIAL (TSINGTAO) CO LTD
View PDF5 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0004] Invention patent CN106943618B provides a wormwood health-care sanitary napkin and its preparation method. In the preparation process, moxa, antibacterial fiber and ES fiber are evenly mixed, and ingredients such as glutinous rice, mint, and persimmon leaves are used together to improve the health care of wormwood. Towel antibacterial effect, however, it does not add natural antibacterial ingredients to ES fibers during the preparation process
During related experiments, the applicant found that plant extracts are not resistant to high temperatures, and when they are melt-blended with ES fibers to prepare fiber products, they are easily charred or lost, reducing their functionality; and the addition of plant extracts will affect ES fibers. The mechanical strength of the fiber, the air permeability of the fiber product, etc.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0028] Embodiment 1 A kind of ES fiber containing wormwood extract and preparation method thereof

[0029] 1. Preparation of functional modifier containing wormwood extract

[0030] Mix the wormwood extract and the porous material and add water to stir and dissolve to form a suspension with a concentration of 8%, and then place it in an ultrasonic pulverizer for processing, and ultrasonicate it at 200MHz for 20min; Homogenize in the quality machine for 8 minutes, dry, and obtain the functional modifier containing the wormwood extract;

[0031] The porous material is a diatomite composite porous material, wherein the mass ratio of alumina, sodium metaaluminate and diatomite is 2:4:18, and the average particle size is 10,000 mesh;

[0032] The mixing mass ratio of the wormwood extract to the porous material is 1:5;

[0033] The accelerator includes propylene glycol alginate, calcium stearate and xanthan gum, the mixing ratio of propylene glycol alginate, calcium stearate and x...

Embodiment 2

[0055] Embodiment 2 A kind of ES fiber containing wormwood extract and preparation method thereof

[0056] 1. Preparation of functional modifier containing wormwood extract

[0057] Mix the wormwood extract and the porous material and add water to stir and dissolve to form a suspension with a concentration of 12%, which is then placed in an ultrasonic pulverizer for processing, and ultrasonicated for 30 minutes at 250 MHz; Homogenized treatment in a quality machine for 10 minutes, drying, to obtain a functional modifier containing wormwood extract;

[0058] The porous material is a diatomite composite porous material, wherein the mass ratio of alumina, sodium metaaluminate and diatomite is 3:5:16, and the average particle size is 10,000 mesh;

[0059] The mixing mass ratio of the wormwood extract to the porous material is 1:8;

[0060] The accelerator includes propylene glycol alginate, calcium stearate and xanthan gum, the mixing ratio of propylene glycol alginate, calcium ...

Embodiment 3

[0082] Embodiment 3 A kind of ES fiber containing wormwood extract and preparation method thereof

[0083] 1. Preparation of functional modifier containing wormwood extract

[0084] Mix the wormwood extract and the porous material and add water to stir and dissolve to form a suspension with a concentration of 15%, which is then placed in an ultrasonic pulverizer for processing, and ultrasonicated at 300MHz for 30 minutes; an accelerator is added to it, and then transferred to a high-pressure homogenizer. Homogenized treatment in a quality machine for 10 minutes, drying, to obtain a functional modifier containing wormwood extract;

[0085] The porous material is a diatomite composite porous material, wherein the mass ratio of alumina, sodium metaaluminate and diatomite is 4:5:20, and the average particle size is 12000 mesh;

[0086] The mixing mass ratio of the wormwood extract to the porous material is 1:10;

[0087] The accelerator includes propylene glycol alginate, calciu...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
melting pointaaaaaaaaaa
densityaaaaaaaaaa
melt flow indexaaaaaaaaaa
Login to View More

Abstract

The invention provides an ES fiber containing a wormwood extract and a preparation method thereof. The content of the wormwood extract in the ES fiber is 0.1-5%, and the preparation method comprises the preparation of a functional modifier containing the wormwood extract, The preparation of the cortex material, the preparation of the core material, composite spinning and post-treatment, the ES fiber containing the wormwood extract prepared by this method has a natural antibacterial effect, and the antibacterial rate against Escherichia coli is 96.5-99.2%. The antibacterial rate against Staphylococcus aureus is 95.0-97.2%, and the antibacterial rate against Candida albicans is 94.5-96.0%. At the same time, the fiber density of this ES fiber is 0.98-1.20g / cm3, and the fineness is 1.2-1.6dtex. The breaking strength reaches 6.2cN / dtex-6.6cN / dtex, and the breaking elongation is 4.5-6.0%. This new type of composite fiber has excellent comprehensive properties.

Description

technical field [0001] The invention belongs to the technical field of ES fiber and its preparation, and in particular relates to an ES fiber containing wormwood extract and a preparation method thereof. Background technique [0002] ES fiber is an eye-catching polyolefin fiber developed by Chisso Corporation of Japan. It is a new type of thermal bonding composite fiber. Nonwoven molded body. ES fiber is made by combining two resins with different melting points. Using the difference in melting point between the two, the bonding between fibers can be achieved only through heat treatment. Because it is a clean fiber without using a binder, the ES fiber cross section The form is "skin-core type" or "side-by-side type", which has a wide range of processing suitability. The non-woven fabric processed by ES fiber has good bulkiness, softness and wet elasticity, and is widely used on the surface of sanitary products. layer. [0003] In the existing technology, the application r...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): D01F8/06D01F1/10D01D5/34
CPCD01D5/34D01F1/10D01F1/103D01F8/06
Inventor 黄效华刘洁刘宇甄丽黄效谦
Owner BESTEE MATERIAL (TSINGTAO) CO LTD
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products