Fire extinguishing agent composition and preparation method and application thereof
The technology of a composition and fire extinguishing agent, which is applied in the field of fire extinguishing agent composition and its preparation and application, can solve the problems of poor cooling effect of water-based fire extinguishing agents, and achieve the effects of protecting life and property, simple preparation method, and reducing surface tension
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] This embodiment discloses a preparation method of a fire extinguishing agent composition, comprising the following steps:
[0030] In the reaction kettle, add 12.5kg Dupont fluorocarbon surfactant 1115, 6.25kg stearic acid, 3.125kg cocamidopropyl betaine, 3.125kg alkyl glycoside APG 0810 in 460kg water, and stir at 80rpm for 20min to dissolve and form a homogeneous phase Surfactant solution;
[0031] Add 35kg of silicone resin polyether emulsion MPS into 460kg of water, stir at 80rpm for 20min to dissolve to obtain a foam stabilizer solution;
[0032] Add the foam stabilizer solution into the surfactant solution, stir at 80rpm for 20min and dissolve to form a clear and uniform mixed solution;
[0033] Stir 20 kg of sodium lauryl sulfate at 60 rpm for 10 min, add it into the mixed solution, and stir at 80 rpm for 50 min to dissolve to obtain the fire extinguishing agent composition.
Embodiment 2
[0035] This embodiment discloses a preparation method of a fire extinguishing agent composition, comprising the following steps:
[0036] In the reaction kettle, add 20kg of Dupont fluorocarbon surfactant 1115, 6kg of stearic acid, 1kg of cocamidopropyl betaine, 2kg of lecithin, 3kg of alkyl glycoside APG 0810 in 460kg of water, and stir at 100rpm for 30min to dissolve and form a homogeneous phase Surfactant solution;
[0037] Add 30kg of silicone resin polyether emulsion (MPS) into 460kg of water, stir at 100rpm for 30min and dissolve to obtain a foam stabilizer solution;
[0038] Add the foam stabilizer solution into the surfactant solution, stir at 80rpm for 30min and dissolve to form a clear and uniform mixed solution;
[0039] Stir 15kg of fatty alcohol polyoxyethylene ether sodium sulfate at 55rpm for 15min, add it into the mixed solution, stir at 80rpm for 50min and dissolve to obtain the fire extinguishing agent composition.
Embodiment 3
[0041] This embodiment discloses a preparation method of a fire extinguishing agent composition, comprising the following steps:
[0042] In the reaction kettle, add 10kg DuPont fluorocarbon surfactant 1115, 5kg sodium dodecylbenzene sulfonate, 5kg cocamidopropyl betaine, 2kg alkyl glycoside APG 0810, 3kg fatty acid glyceride, 100rpm in turn in 460kg water Stir for 50min to dissolve and form a homogeneous surfactant solution;
[0043]Add 30kg of silicone resin polyether emulsion (MPS) into 460kg of water, stir at 100rpm for 50min and dissolve to obtain a foam stabilizer solution;
[0044] Add the foam stabilizer solution into the surfactant solution, stir at 80rpm for 30min and dissolve to form a clear and uniform mixed solution;
[0045] 15kg of sodium lauryl sulfate and 10kg of fatty alcohol polyoxyethylene ether sodium sulfate were stirred at 60 rpm for 10 minutes, added into the mixed solution, stirred at 80 rpm for 50 minutes and dissolved to obtain the fire extinguishin...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com