Preparation method and applications of self-cleaning aqueous high-gloss varnish
A self-cleaning, water-based technology, applied in the direction of coatings, polyurea/polyurethane coatings, etc., can solve the problems of leveling, construction that cannot meet people's needs, poor permeability, easy to wear, etc., and achieve hardness Good, fast drying at room temperature, flexible and impact-resistant paint film
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] A kind of preparation method of self-cleaning type water-based high-gloss varnish proposed by the present invention comprises the following concrete steps:
[0026] S1. Weigh the following raw materials by weight: 60 parts of water-based acrylic resin emulsion, 15 parts of water-based polyurethane resin, 0.1 part of wetting agent, 0.2 part of leveling agent, 0.1 part of defoaming agent, 3 parts of film-forming aid, hand wax 1 part of slurry, 0.1 part of preservative, 0.1 part of pH regulator, 0.3 part of thickener, 0.1 part of bactericide, 0.1 part of ultraviolet absorber, 10 parts of deionized water, 60 parts of hydrophilic polyisocyanate, propylene glycol diacetic acid 20 parts of ester and 0.1 part of adhesion promoter;
[0027] S2. Add water-based acrylic resin emulsion, wetting agent, leveling agent, defoamer, bactericide, ultraviolet absorber, and hand wax slurry into a high-speed mixer, and stir at a speed of 1000-1500r / min for 10-20min to obtain a mixture A;
...
Embodiment 2
[0043] A kind of preparation method of self-cleaning type water-based high-gloss varnish proposed by the present invention comprises the following concrete steps:
[0044] S1. Weigh the following raw materials by weight: 70 parts of water-based acrylic resin emulsion, 30 parts of water-based polyurethane resin, 0.3 part of wetting agent, 0.4 part of leveling agent, 0.4 part of defoaming agent, 9 parts of film-forming aid, hand wax 4 parts of pulp, 0.4 parts of preservative, 0.3 parts of pH regulator, 0.4 parts of thickener, 0.3 parts of bactericide, 0.5 parts of ultraviolet absorber, 30 parts of deionized water, 70 parts of hydrophilic polyisocyanate, propylene glycol diacetic acid 40 parts of ester and 0.4 part of adhesion promoter;
[0045] S2. Add water-based acrylic resin emulsion, wetting agent, leveling agent, defoamer, bactericide, ultraviolet absorber, and hand wax slurry into a high-speed mixer, and stir for 14 minutes at a speed of 1200r / min to obtain a mixture A;
...
Embodiment 3
[0061] A kind of preparation method of self-cleaning type water-based high-gloss varnish proposed by the present invention comprises the following concrete steps:
[0062] S1. Weigh the following raw materials by weight: 90 parts of water-based acrylic resin emulsion, 40 parts of water-based polyurethane resin, 0.5 part of wetting agent, 0.8 part of leveling agent, 0.6 part of defoamer, 15 parts of film-forming aid, hand wax 6 parts of slurry, 0.6 parts of preservative, 0.4 parts of pH regulator, 0.9 parts of thickener, 0.6 parts of bactericide, 0.8 parts of ultraviolet absorber, 40 parts of deionized water, 80 parts of hydrophilic polyisocyanate, propylene glycol diacetic acid 50 parts of ester and 0.6 parts of adhesion promoter;
[0063] S2. Add water-based acrylic resin emulsion, wetting agent, leveling agent, defoamer, bactericide, ultraviolet absorber, and hand wax slurry into a high-speed mixer, and stir for 20 minutes at a speed of 1500r / min to obtain a mixture A;
[0...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com