A manufacturing method and stack technology, applied in the field of manufacturing, can solve problems affecting the performance and operating life of the stack, affect the assembly effect, and have high requirements, so as to improve the success rate and efficiency of assembly, reduce uncertain factors, and solve technical problems. The effect of defects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] Embodiment 1, manufacture 20kw stack module
[0014] 1) According to the drawing design, produce a 20kw electric stack, the width of the cathode and anode sealing grooves of the bipolar plates of the electric stack is 4mm, the groove depths are 0.5mm and 0.3mm respectively, the effective area of the membrane electrode is 230cm2, and the thickness of the membrane electrode edge protection is 0.125mm PET material, the membrane electrode edge protection thickness after packaging is 0.25mm.
[0015] 2) Use a precision online dispensing machine to perform dispensing operations on the cathode and anode sealing grooves of the bipolar plate. The glue used is polyolefin glue. The width of the cathode dispensing is 3mm, the height is 0.6mm, and the width of the anode dispensing is 3mm, height 0.4mm.
[0016] 3) Assembling a 20kw electric stack requires 136 single cells. The 136 bipolar plates and membrane electrodes are cross-stacked according to the sandwich structure, and a ...
Embodiment 2
[0018] Embodiment 2, manufacture 36kw stack module
[0019] 1) According to the blueprint design, produce a 36kw electric stack module, the average width of the cathode and anode sealing grooves of the electric stack bipolar plate is 3.5mm, the groove depth is 0.4mm, the effective area of the membrane electrode is 330cm2, and the membrane electrode edge protection material is 0.15mm thick PEN material, the membrane electrode edge protection thickness after packaging is 0.3mm. The size of the bipolar plate is 340*150mm, and a 0.8mm hole is processed in the middle of the short sides on both sides of the bipolar plate, and the hole is respectively connected with the sealing groove of the cathode and anode.
[0020] 2) Assembling a 36kw electric stack requires 170 single cells. The 170 bipolar plates and membrane electrodes are cross-stacked according to the sandwich structure, and a pressure of about 2100kg is applied. At this time, the thickness of the electric stack will not ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com