Embodiment 1
[0077] (1) put 5000Nm 3 / h of the first flue gas (900°C) indirectly heats 4,500kg of raw coal (lignite, with a particle size of 20mm) in the rotary kiln for 45 minutes of coal conversion, and the final conversion temperature is 600°C to obtain the first flue gas, the first pyrolysis gas and converted coal;
[0078] (2) put 5000Nm 3 / h of the second flue gas (900°C) indirectly heats the converted coal in the rotary kiln to remove impurities for 35 minutes. ;
[0079] (3) dry-cooling the de-miscellaneous coal to obtain clean coal;
[0080](4) After the first and second pyrolysis gases are combined, the tar is removed to obtain a tar product; at the same time, the obtained coal gas is passed into a co-firing furnace for combustion, and the obtained hot air is passed into a waste heat boiler to exchange heat with boiler feed water to generate steam And tail gas, steam (temperature 800°C) is returned to the power plant boiler for power generation, and the tail gas is used as re...
Embodiment 2
[0084] (1) Use 6500Nm 3 / h of the first flue gas (1000°C) indirectly heats 4000kg of raw coal (non-caking coal, particle size: 30mm) in the tower moving bed to carry out coal conversion for 30min, and the final conversion temperature is 500°C to obtain the first flue gas, first pyrolysis gas and converted coal;
[0085] (2) Use 3500Nm 3 / h of the second flue gas (1000°C) indirectly heats the converted coal in the rotary kiln to remove impurities for 30 minutes, and the final removal temperature is 700°C to obtain the second flue gas, the second pyrolysis gas and the coal;
[0086] (3) dry-cooling the de-miscellaneous coal to obtain clean coal;
[0087] (4) After the first and second pyrolysis gases are combined, the tar is removed to obtain a tar product; at the same time, the obtained coal gas is passed into a co-firing furnace for combustion, and the obtained hot air is passed into a waste heat boiler to exchange heat with boiler feed water to generate steam And tail gas...
Embodiment 3
[0091] (1) Use 6000Nm 3 / h of the first flue gas (950°C) indirectly heats 5000kg of raw coal (long-flame coal, particle size: 3mm) in the tower-type moving bed, and carries out coal conversion for 40min, and the final conversion temperature is 550°C, and the first flue gas, first pyrolysis gas and converted coal;
[0092] (2) with 4000Nm 3 The first flue gas (950°C) in the rotary kiln indirectly heats the converted coal in the rotary kiln for 30 minutes of coal removal, and the final removal temperature is 650°C to obtain the second flue gas, the second pyrolysis gas and the removal of impurities coal;
[0093] (3) dry-cooling the de-miscellaneous coal to obtain clean coal;
[0094] (4) After the first and second pyrolysis gases are combined, the tar is removed to obtain a tar product; at the same time, the obtained coal gas is passed into a co-firing furnace for combustion, and the obtained hot air is passed into a waste heat boiler to exchange heat with boiler feed water ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com