Ultra-micro powder plant slice and preparation method thereof
A plant and powder technology, which is applied in the fields of tobacco preparation, food science, and application, can solve the problems of complex process, small smoke volume, and low utilization rate of raw materials for aroma production.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0066] Embodiment 1: the preparation of ultrafine powder plant flakes
[0067] The preparation steps of this preparation method are as follows:
[0068] A. Outer edge fiber cutting
[0069] Add 20 parts by weight of water to 5 parts by weight of the bamboo pulp fiber outer edge fiber, then use a mixer to stir for 34min at a speed of 23rpm, stir evenly, and obtain the outer edge fiber shear fiber slurry;
[0070] B. Preparation of colloidal viscous fluid
[0071] Take by weighing 70 parts by weight of flue-cured tobacco plant superfine powder with a particle size of 120 objects, 3 parts by weight of guar gum binder and 20 parts by weight of glycerol fuming agent, and add them to the outer edge fiber shear fiber pulp obtained in step A In the liquid, use a stirrer to stir for 17 minutes under the condition of a rotating speed of 25rpm, and stir evenly to obtain a colloidal viscous fluid;
[0072] C. Forming of plant flakes
[0073] Using a screw extrusion device, evenly spre...
Embodiment 2
[0076] Embodiment 2: the preparation of ultrafine powder plant flakes
[0077] The preparation steps of this preparation method are as follows:
[0078] A. Outer edge fiber cutting
[0079] Add 30 parts by weight of water to 8 parts by weight of the wood pulp fiber outer edge fiber, then use a mixer to stir for 20 minutes at a speed of 24 rpm, and stir evenly to obtain the outer edge fiber shear fiber slurry;
[0080] B. Preparation of colloidal viscous fluid
[0081] Take by weighing 80 parts by weight of mint plant superfine powder, 2 parts by weight of shellac binder and 14 parts by weight of glyceryl diacetate fuming agent respectively, and add them to the outer edge fiber shear fiber pulp obtained in step A In the liquid, use a stirrer to stir for 15 minutes under the condition of a rotating speed of 50rpm, and stir evenly to obtain a colloidal viscous fluid;
[0082] C. Forming of plant flakes
[0083] Using a screw extrusion device, evenly spread the colloidal visco...
Embodiment 3
[0086] Embodiment 3: the preparation of superfine powder plant flakes
[0087] The preparation steps of this preparation method are as follows:
[0088] A. Outer edge fiber cutting
[0089] Add 25 parts by weight of water to 3 parts by weight of sugarcane fiber outer edge fibers, then use a mixer to stir for 30 minutes at a speed of 35 rpm, stir evenly, and obtain outer edge fiber shear fiber slurry;
[0090] B. Preparation of colloidal viscous fluid
[0091] Take 85 parts by weight of tea plant superfine powder with a particle size of 220 objects, 2 parts by weight of CMC binder and 30 parts by weight of triacetin fuming agent, and add them to the outer edge fiber shear pulp obtained in step A In the liquid, use a stirrer to stir for 18 minutes under the condition of a rotating speed of 20rpm, and stir evenly to obtain a colloidal viscous fluid;
[0092] C. Forming of plant flakes
[0093] Using a screw extrusion device, the colloidal viscous fluid obtained in step B is e...
PUM
Property | Measurement | Unit |
---|---|---|
Granularity | aaaaa | aaaaa |
Thickness | aaaaa | aaaaa |
Gram weight | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com