an altered flute
A flute and flute pipe technology, applied in the field of musical instruments, can solve the problems of poor flute changing effect, etc., and achieve the effect of hard texture, improved control ability, and bright sound.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0029] An altered flute, including a flute tube and keys, wherein the flute tube includes a flute head, a flute body and a flute tail, and the flute tube part is provided with a blow hole, a sound hole and a flute plug, and the flute tube is made of aluminum metal. Diameter D is 1.5cm, and the length L=30D of flute tube, take the central line of blow hole as reference, the film material of nanotube coating on the inner surface of the flute part of front and rear 3cm, the thickness of film is 300nm.
[0030] The coating process is as follows: disperse 100 mg of commercially available carbon nanotubes in 30 g of deionized water, add 200 mg of dispersant sodium lauryl sulfate, and ultrasonically disperse; place the dispersed carbon nanotubes in the top loading liquid of the spray gun In the cup, adjust the pressure of the nitrogen cylinder and the outlet of the spray gun, and use nitrogen to send the liquid, so that the carbon nanotube dispersion becomes a mist through the spray g...
Embodiment 2
[0033]An altered flute, including a flute tube and keys, wherein the flute tube includes a flute head, a flute body and a flute tail. Diameter D is 2cm, and the length L=33D of flute tube, take the centerline of blow hole as reference, the film material of nanotube coating on the inner surface of the flute part of front and rear 3cm, the thickness of film is 200nm.
[0034] The coating process is: disperse commercially available titanium dioxide nanotubes in 100 mg in 30 g of deionized water, add 200 mg of dispersant sodium lauryl sulfate, and ultrasonically disperse; place the dispersed carbon nanotubes in the top loading liquid of the spray gun In the cup, adjust the pressure of the nitrogen cylinder and the outlet of the spray gun, and use nitrogen to send the liquid, so that the carbon nanotube dispersion becomes a mist through the spray gun for spraying. During the spraying process, the temperature of the pipe is maintained at about 100 °C.
[0035] When the obtained flut...
Embodiment 3
[0037] An altered flute, including a flute tube and keys, wherein the flute tube includes a flute head, a flute body and a flute tail. The diameter D is 2cm, and the length L of the flute tube is 33D. Taking the center line of the blowing hole as the reference, the inner surface of the front and back 3cm flute tube part is coated with a thin film material of nanotubes. The thickness of the film is 200nm. The coating process uses electroplating coated.
[0038] When the obtained flute is played, it is easy to control the number of harmonics when playing, and to realize the change of timbre.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com