Electric wire cable used for aerospace and preparation method thereof
An aerospace, wire and cable technology, applied to rubber insulators, organic insulators, etc., can solve the problems of long preparation time, uneven performance of rubber products, uneven mixing, etc., to reduce the risk of raw material aging, high promotion and application value, The effect of increasing the production efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0014] The invention provides a method for preparing wires and cables for aerospace, including the steps of assembling an inner conductor, an insulating layer, an outer conductor layer, a water blocking layer and a sheath sequentially from the inside to the outside, wherein the sheath The preparation method comprises the following steps: (1) mixing ceramic fibers with a silane coupling agent to obtain a pretreatment reinforcing agent; (2) mixing polyvinyl acetate, a first solvent, fluororubber, carbon black, a pretreatment reinforcing agent, Zinc, molybdenum series catalyst and anti-aging agent carry out banburying once, then leave standstill; (3) add the second solvent, white carbon black and vulcanizing agent in the first banbury after standing and carry out second banbury; (4) with The total amount of solvent formed by the first solvent and the second solvent is 100%, and the secondary banburying product is flash evaporated to remove 70-90% of the solvent; (5) the flash evap...
preparation example 1
[0043] The ceramic fiber and the silane coupling agent were mixed for 50 minutes at 180°C with a rotation speed of 800rpm, wherein the weight ratio of the ceramic fiber to the silane coupling agent was 1:1, and the silane coupling agent was a mixture of KH550 and KH570, wherein, The weight ratio of KH550 and KH570 is 1:2 to obtain pretreatment enhancer.
preparation example 2
[0045] The ceramic fiber and the silane coupling agent were mixed for 30 minutes at 120°C with a rotation speed of 500rpm, wherein the weight ratio of the ceramic fiber to the silane coupling agent was 1:3, and the silane coupling agent was a mixture of KH550 and KH570, wherein, The weight ratio of KH550 and KH570 is 1:3 to obtain pretreatment enhancer
PUM
Property | Measurement | Unit |
---|---|---|
particle size (mesh) | aaaaa | aaaaa |
particle size (mesh) | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com