Water-soluble ink printing process for woven bags
A technology of ink printing and woven bags, which is applied in printing, ink, printing machines, etc., can solve problems such as inaccurate color registration, printing, and harm to human body, and achieve the effect of fast printing speed, large printing volume, and exquisite quality
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0040] A water-soluble ink printing process for woven bags, comprising the following steps:
[0041] (1) plate making
[0042] Choose a carving needle or a carving knife to carve the gravure plate, the opening size of the gravure plate mesh is 105 μm, and the depth of the gravure plate is 28 μm;
[0043] (2) Ink adjustment
[0044] The ink components and mass percentages of inks used in plastic woven bag printing are as follows:
[0045] Acrylic acid addition rosin resin: 51%;
[0046] Non-toxic pigments: 9.5%;
[0047] Ammonia: 9%;
[0048] Pure acrylic emulsion: 12%;
[0049] Water-based wax: 3.4%;
[0050] Defoamer: 0.2%;
[0051] Leveling agent: 0.4%;
[0052] Water: 14.5%;
[0053] Add ammonia water to acrylic acid addition rosin resin for amination treatment, the pH value of the solution after amination is 7.8, mix the solution after amination with non-toxic pigment, pure acrylic emulsion, water-based wax, water defoamer, leveling Fully mix the agent and water ...
Embodiment 2
[0071] A water-soluble ink printing process for woven bags, comprising the following steps:
[0072] (1) plate making
[0073] Choose a carving needle or a carving knife to carve the gravure plate. The opening size of the gravure plate is 125 μm, and the depth of the gravure plate is 33 μm;
[0074] (2) Ink adjustment
[0075] The ink components and mass percentages of inks used in plastic woven bag printing are as follows:
[0076] Acrylic acid addition rosin resin: 52%;
[0077] Non-toxic pigments: 8.5%;
[0078] Ammonia: 9.9%;
[0079] Pure acrylic emulsion: 11%;
[0080] Water-based wax: 5%;
[0081] Defoamer: 0.6%;
[0082] Leveling agent: 0.5%;
[0083] Water: 12.5%;
[0084]Add ammonia water to acrylic acid addition rosin resin for amination treatment, the pH value of the aminated solution is 8.3, mix the aminated solution with non-toxic pigments, pure acrylic emulsion, water-based wax, water defoamer, leveling Fully mix the agent and water to make it evenly d...
Embodiment 3
[0102] A water-soluble ink printing process for woven bags, comprising the following steps:
[0103] (1) plate making
[0104] Choose a carving needle or a carving knife to carve the gravure plate, the opening size of the gravure plate mesh is 115 μm, and the depth of the gravure plate is 30 μm;
[0105] (2) Ink adjustment
[0106] The ink components and mass percentages of inks used in plastic woven bag printing are as follows:
[0107] Acrylic acid addition rosin resin: 51.3%;
[0108] Non-toxic pigments: 8.6%;
[0109] Ammonia: 11%;
[0110] Pure acrylic emulsion: 11.2%;
[0111] Water-based wax: 3.2%;
[0112] Defoamer: 0.9%;
[0113] Leveling agent: 0.8%;
[0114] Water: 13%;
[0115] Add ammonia water to acrylic acid addition rosin resin for amination treatment, the pH value of the solution after amination is 8, mix the solution after amination with non-toxic pigment, pure acrylic emulsion, water-based wax, water defoamer, leveling Fully mix the agent and water...
PUM
Property | Measurement | Unit |
---|---|---|
length | aaaaa | aaaaa |
width | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com