Two-component waterborne colorful paint coating
A multi-color paint, two-component technology, applied in multi-color effect coatings, fireproof coatings, polyurea/polyurethane coatings, etc., can solve the problems of poor water resistance, stain resistance and scrub resistance, inconvenient construction, and low service life. problem, to achieve the effect of stable composition, long shelf life at room temperature, and good adhesion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] Add deionized water, water-based hydroxyl dispersion, defoamer, dispersant, pigment filler and preservative into the dispersion container, disperse at a high speed of 15 m / s for 22 minutes, then add anti-settling agent, pH value stabilizer, resin and Curing agent, stir at 7 m / s for 13 minutes to obtain component A, then mix component B and component A, the ratio between component A and component B is 3:2, and stir evenly to obtain The two-component water-based polychrome paint.
[0021] In this example, deionized water: 19 parts; dispersant: 0.5 parts; anti-settling agent: 1 part, the anti-settling agent is modified polyamide wax; preservative: 0.8 parts; pH stabilizer: 0.4 parts, the pH stabilizer is 2-amino-2-methyl-1-propanol; defoamer: 0.1 parts; pigments and fillers: 15 parts, the pigments and fillers include titanium dioxide, diatomaceous earth and dioxide Silicon; water-based hydroxyl dispersion: 69 parts; resin: 42 parts, the resin is water-based hydroxyl resin...
Embodiment 2
[0023] Add deionized water, water-based hydroxyl dispersion, defoamer, dispersant, pigment and filler and preservative into the dispersion container, disperse at a high speed of 10 m / s for 18 minutes, then add anti-settling agent, pH value stabilizer, resin and Curing agent, stir at 4 m / s for 9 minutes to obtain component A, then mix component B and component A, the ratio between component A and component B is 3:2, and stir evenly to obtain The two-component water-based polychrome paint.
[0024] In this embodiment, deionized water: 15 parts; dispersant: 0.3 parts; anti-settling agent: 2 parts, the anti-settling agent is modified polyamide wax; preservative: 1 part; pH stabilizer: 0.2 parts, the pH stabilizer is 2-amino-2-methyl-1-propanol; defoamer: 0.3 parts; pigments and fillers: 12 parts, the pigments and fillers include titanium dioxide, diatomaceous earth and dioxide Silicon; water-based hydroxyl dispersion: 61 parts; resin: 49 parts, the resin is water-based hydroxyl r...
Embodiment 3
[0026] Add deionized water, water-based hydroxyl dispersion, defoamer, dispersant, pigment filler and preservative into the dispersion container, disperse at a high speed of 12 m / s for 20 minutes, then add anti-settling agent, pH value stabilizer, resin and Curing agent, stir at 5 m / s for 11 minutes to obtain component A, then mix component B and component A, the ratio between component A and component B is 3:2, and stir evenly to obtain The two-component water-based polychrome paint.
[0027] In this embodiment, deionized water: 17.5 parts; dispersant: 0.4 parts; anti-settling agent: 1.5 parts, the anti-settling agent is modified polyamide wax; preservative: 0.9 parts; pH stabilizer: 0.3 parts, the pH stabilizer is 2-amino-2-methyl-1-propanol; defoamer: 0.2 parts; pigments and fillers: 14 parts, the pigments and fillers include titanium dioxide, diatomaceous earth and dioxide Silicon; water-based hydroxyl dispersion: 65 parts; resin: 45 parts, the resin is water-based hydrox...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com