Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

A kind of method utilizing chromium-containing Glauber's salt to prepare anhydrous sodium sulfate

A technology of anhydrous sodium sulfate and mirabilite, which is applied in chemical instruments and methods, alkali metal sulfites/sulfites, chromium compounds, etc. Chromium exceeding the standard and other problems, to achieve the effect of facilitating automatic continuous production, promoting the optimization of product structure, and reducing production costs

Active Publication Date: 2019-11-29
陕西省商南县东正化工有限责任公司
View PDF2 Cites 2 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0002] Before 2000, the total annual production of sodium dichromate in my country's chromium salt enterprises was less than 100,000 tons, and the total amount of by-product chromium-containing Glauber's salt was about 130,000 tons. Sodium sulfate water, but due to the small production scale of sodium dichromate and the low output of by-product chromium-containing Glauber's salt, the cost of using chromium-containing Glauber's salt to prepare industrial anhydrous sodium sulfate is higher than the cost of directly using natural Glauber's salt to produce anhydrous sodium sulfate. This kind of research was terminated, and the dried chromium-containing Glauber's salt was used as the cement accelerator instead. Since the hexavalent chromium in the chromium-containing Glauber's salt has not been reduced, the cement accelerator made will pollute the environment
In the end, most chromium salt manufacturers choose to use chromium-containing Glauber's salt to produce soda sulfide, because the hexavalent chromium in chromium-containing Glauber's salt will be reduced to detoxify during the production of soda sulfide, but the waste gas and slag generated during the production of soda sulfide are still in polluted environment
[0003] After 2000, research on the reuse of chromium-containing Glauber's salt gradually emerged. Sichuan Anxian Yinhe Jianhua Group Co., Ltd. developed a method for preparing potassium sulfate from chromium-containing Glauber's salt (CN200610000019.1), but due to high energy consumption, It is difficult to achieve continuous production, resulting in high production costs of potassium sulfate, unable to form market competitiveness
In recent years, Li Xianrong, Hu Yihua and others of Sichuan Yinhe Chemical Co., Ltd. have developed a method for refining sodium sulfate by chromium-containing Glauber's salt (CN201310533304.X). This method uses the crystal slurry method to produce sodium sulfate, but Due to the problem of hexavalent chromium wrapped in crystal slurry, the hexavalent chromium in the produced sodium sulfate exceeds the standard, sometimes as high as 100ppm; and because the process does not remove impurities and decolorize, the whiteness of the product cannot meet GB / T 6009-2014 Industrial anhydrous sodium sulfate standard requirement; In addition, the reducing agent that adopts in this method is sodium sulfite, and neutralizing agent is caustic soda, and these two kinds of raw materials are too expensive for low-value product sodium sulfate, cause the cost of sodium sulfate produced Too high, patented technology cannot form actual productivity

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0039] Utilize the method for preparing anhydrous sodium sulfate by chromium-containing Glauber's salt, comprising the following steps:

[0040] (1) dissolving chromium-containing Glauber's salt in chromium-containing aluminum mud washing water to obtain chromium-containing Glauber's salt aqueous solution, and controlling the concentration of sodium sulfate in the gained chromium-containing Glauber's salt aqueous solution to be 15%;

[0041] (2) Add quantitative sodium thiosulfate to the chromium-containing Glauber’s salt aqueous solution, the molar ratio of hexavalent chromium to sodium thiosulfate is 1:2.7, and under the conditions of 0.3Mpa and 130°C, hexavalent chromium is Reduced to trivalent chromium, precipitated in the form of hydrated chromium oxide;

[0042] (3) Neutralize the reduced chromium-containing Glauber's salt aqueous solution with industrial sulfuric acid, control the pH value to 7, and control the temperature at 95°C to promote the precipitation of water-s...

Embodiment 2

[0048] Utilize the method for preparing anhydrous sodium sulfate by chromium-containing Glauber's salt, comprising the following steps:

[0049] (1) dissolving chromium-containing Glauber's salt in chromium-containing Glauber's salt washing water to obtain chromium-containing Glauber's salt aqueous solution, and controlling the concentration of sodium sulfate in the gained chromium-containing Glauber's salt aqueous solution to be 20%;

[0050] (2) Add quantitative sodium thiosulfate to the chromium-containing Glauber’s salt aqueous solution, the molar ratio of hexavalent chromium to sodium thiosulfate is 1:3.0, and under the conditions of 0.2Mpa and 120°C, the hexavalent chromium is Reduced to trivalent chromium, precipitated in the form of hydrated chromium oxide;

[0051] (3) Neutralize the reduced chromium-containing Glauber's salt aqueous solution with industrial sulfuric acid, control the pH value to 6.7, and control the temperature at 80°C to promote the precipitation of...

Embodiment 3

[0057] Utilize the method for preparing anhydrous sodium sulfate by chromium-containing Glauber's salt, comprising the following steps:

[0058] (1) dissolving chromium-containing Glauber's salt in evaporated chromium-containing condensed water to obtain chromium-containing Glauber's salt aqueous solution, and controlling the concentration of sodium sulfate in the gained chromium-containing Glauber's salt aqueous solution to be 25%;

[0059] (2) Add quantitative sodium thiosulfate to the aqueous solution of chromium-containing Glauber’s salt, the molar ratio of hexavalent chromium to sodium thiosulfate is 1:2.8, and at 0.2Mpa and 120°C, hexavalent chromium is Reduced to trivalent chromium, precipitated in the form of hydrated chromium oxide;

[0060] (3) Neutralize the reduced chromium-containing Glauber's salt aqueous solution with industrial sulfuric acid, control the pH value to 7, and control the temperature at 100°C to promote the precipitation of water-soluble trivalent ...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention relates to the field of a chemical industry and particularly relates to a method for preparing anhydrous sodium sulfate from chromium-containing mirabilite as a by-product in the production process of sodium dichromate. The method comprises dissolving a certain concentration of chrome-containing mirabilite in chromium-containing waste water, adding quantitative sodium thiosulfate into the waste water to promote reduction of hexavalent chromium into trivalent chromium under 0.1-1 Mpa at 80-190 DEG C, wherein the trivalent chromium in a form of chromium trioxide hydrate is precipitated, adding a small amount of sulfuric acid to neutralize, filtering to acquire the chromium trioxide hydrate, removing impurities, carrying out decoloration, evaporating to precipitate anhydrous sodium sulfate crystals, and carrying out continuous centrifugal separation and drying. The method is simple and easy, utilizes cheap raw materials, has low energy consumption and a high automation degree and is suitable for large-scale production. The quality of the industrial anhydrous sodium sulfate product obtained by the method meets the requirements of class I products in the GB / T 6009-2014 industrial anhydrous sodium sulfate standard.

Description

technical field [0001] The invention relates to the field of chemical industry, in particular to a method for preparing anhydrous sodium sulfate by utilizing chromium-containing Glauber's salt, a by-product in the production process of sodium dichromate. Background technique [0002] Before 2000, the total annual production of sodium dichromate in my country's chromium salt enterprises was less than 100,000 tons, and the total amount of by-product chromium-containing Glauber's salt was about 130,000 tons. Sodium sulfate water, but due to the small production scale of sodium dichromate and the low output of by-product chromium-containing Glauber's salt, the cost of using chromium-containing Glauber's salt to prepare industrial anhydrous sodium sulfate is higher than the cost of directly using natural Glauber's salt to produce anhydrous sodium sulfate. This kind of research was terminated, and the dried chromium-containing Glauber's salt was used as a cement accelerator instead....

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): C01D5/00C01G37/00
CPCC01D5/00C01G37/00C01P2006/65C01P2006/80C01P2006/82
Inventor 张国庆
Owner 陕西省商南县东正化工有限责任公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products