Large-thickness Q500GJCD high-strength steel plate for building structure, and manufacturing method thereof
A technology of building structure and manufacturing method, which is applied in the field of special steel metallurgy, can solve the problems of long production cycle, high production cost, and restrictions on customer use, and achieve the effects of low production cost, short manufacturing cycle and low tensile strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
example 1
[0043] Example 1: The present invention designs and smelts the Q500GJC and Q500GJD thick 370mm continuous casting billets provided by the smelting chemical composition, and produces an example of rolling a 40mm thick steel plate. The continuous casting slab is 370×2300×3200mm, and the rolled finished plate is 40×2500×L (length) mm. The billet is cold loaded into the heating furnace, the temperature of the preheating section of the heating furnace: 750-900℃, the temperature of the heating section: 1000-1150℃, the temperature of the second heating section: 1210-1230℃, the temperature of the soaking section: 1200-1220℃; Total time 375 minutes. After rough rolling, the thickness of the waiting temperature is 88mm; after warming, the starting temperature of the finishing mill is 820°C, and the finishing rolling temperature is 815°C; after the rolling is completed, the rolled piece is directly sent to the Acc equipment for watering to accelerate cooling , the cooling rate is 12-13°...
example 2
[0044] Example 2: The present invention designs and smelts Q500GJC and Q500GJD thick 150mm continuous casting billets provided by smelting chemical components, and produces an example of rolling 12mm thick steel plates. The continuous casting slab is 150×2500×3300mm, and the rolled finished plate is 12×2800×L (length) mm. The billet is cold-loaded into the heating furnace, and the heating process is the same as the example 1. After rough rolling, the thickness of waiting temperature is 50mm. After warming, the starting temperature of finishing mill is 900℃, and then finishing rolling, the final rolling temperature is ≥796℃. After rolling, the rolled piece is directly sent to Acc equipment for watering. Accelerated cooling, the cooling rate is 6-7°C / s, and the final cooling temperature is 690-710°C; then it is leveled by a hot straightening machine; after that, it is sent to a cooling bed for natural cooling, and when it is cooled to 320°C, the off-line stack is slowly cooled; ...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
yield strength | aaaaa | aaaaa |
tensile strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com