A kind of soil coagulant, its preparation method and application
A coagulant and soil technology, applied in the field of materials, can solve problems such as land resources and ecological environment damage, and achieve the effects of expanding the scope of application, strengthening the connection force, and improving water permeability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0025] In the preparation process of soil coagulant, different additives are added according to actual needs to achieve the required performance. Further, in a preferred embodiment of the present invention, the additive further includes at least one of an activator, a coagulant, and a water reducer.
[0026] The activator is used to activate the activity of fly ash, promote the reaction between fly ash and mud or waste soil residue, cement and anhydrite, improve the gelling effect and increase the strength of the gel. In a preferred embodiment of the present invention, the activator is sodium sulfate, sodium silicate or sodium carbonate.
[0027] The coagulant has the characteristics of rapid setting, accelerating coagulation, early strength, and good operability. It can accelerate the hardening speed, mainly promote the hydration reaction, and improve the early strength of the gel. In a preferred embodiment of the present invention, the coagulant is sodium bicarbonate, sodiu...
Embodiment 1
[0035] The present embodiment provides a kind of soil coagulant, by weight percentage, comprising:
[0036] 30% cement, 25% fly ash, 10% anhydrous gypsum, 5% anti-solvent.
[0037] It is mainly made by the following methods:
[0038] The above-mentioned raw materials are weighed, and the raw materials are sieved to obtain fine particle size raw materials. The specific sieve is 200 mesh.
[0039] Add the sieved raw materials into a mixer, and stir for 20 minutes at a speed of 800 rpm.
Embodiment 2
[0041] The present embodiment provides a kind of soil coagulant, by weight percentage, comprising:
[0042] 50% of cement, 45% of fly ash, 25% of anhydrite, and 20% of anti-solvent.
[0043] It is mainly made by the following methods:
[0044] The above-mentioned raw materials are weighed, and the raw materials are sieved to obtain fine particle size raw materials. The specific sieve is 500 mesh.
[0045] Add the sieved raw materials into a mixer, and stir for 40 minutes at a speed of 1200 rpm.
PUM
Property | Measurement | Unit |
---|---|---|
compressive strength | aaaaa | aaaaa |
compressive strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com